Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Electrablend® TPX-HTN-01045 A 40% Carbon Filled

Category Polymer , Thermoplastic , Nylon
Manufacturer Techmer ES
Trade Name Electrablend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Electrablend® TPX-HTN-01045 A 40% Carbon Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 40% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized, High Temperature Strength and LubricatedUL File Number: E157318Information provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
ASTM D792
Water Absorption 0.22 %

@Time 86400 sec
0.22 %

@Time 24.0 hour
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 125
125
ASTM D785
Tensile Strength, Yield 310 MPa
45000 psi
ASTM D638
Elongation at Yield 1.3 %
1.3 %
ASTM D638
Flexural Yield Strength 455 MPa
66000 psi
ASTM D790
Flexural Modulus 31.0 GPa
4500 ksi
ASTM D790
Izod Impact, Notched 0.961 J/cm

@Thickness 3.17 mm
1.80 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 34.2 µm/m-°C
19.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 282 °C
540 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 10000 ohm-cm
10000 ohm-cm
ASTM D257