Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 222 °C | 432 °F | ASTM D789 |
NYCOA ASN 27 300 KNF 30% Glass Fiber Reinforced, Heat Stabilized Nylon 6 Resin NYCOA ASN 27 300 KNF is a 30% glass fiber reinforced, heat stabilized Nylon 6 resin used for injection molding. This grade features excellent strength and stiffness, dimensional stability, and a gre.. |
|||
Melting Point | 222 °C | 432 °F | STN EN 11357-1 |
Plastcom PLASTAMID® 6 BT B 27 PA6 Basic type PA 6 for compounding, for general use. Grade can contain PA 66 up to 5% and TiO2 content up to 0.25 %. Use: automotive, engineering, electrical and consumer-goods industryInformation Prov.. |
|||
Melting Point | 222 °C | 432 °F | STN EN 11357-1 |
Plastcom SLOVAMID® 6 GF 30 AS PA6 reinforced with glass fiber, anti-static agent PA 6 for injection molding, reinforced with 30% glass fiber, contains antistatic agent for moldings used in the automotive, electrical, building, engineering and hobby industry - holders of electric.. |
|||
Melting Point | 222 °C | 432 °F | STN EN 11357-1 |
Plastcom SLOVAMID® 6 NG1 GF 30 HLS PA6 reinforced with glass fiber, UV stabilized, hydrolysis resistant PA 6 for injection molding, reinforced with 30% glass fiber, for moldings used in the automotive, weather and UV stabilized. Determined for using in outside automotive applications like door handle,.. |
|||
Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
Lanxess Durethan® B 31 F 000000 Nylon 6, Film Grade PA 6, film grade, low viscosity, easy flow, additive-freeApplication Examples: flat and blown film, monofilaments, coatings |
|||
Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
Lanxess Durethan® B 38 FKA 000000 Nylon 6, Film Grade PA 6 film-grade, medium to higher viscosity, with processing aid and slip agent, nucleated, in compliance with FDA for food contactApplication Examples: flat and blown film, flat film coextrusion fo.. |
|||
Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
Lanxess Durethan® B 40 FA 000000 Nylon 6, Film Grade PA 6, film grade of high viscosity, lubricated, not nucleated, in compliance with FDA for food contact and acc. the German BgVV Recommendation XLIV, Section VI.A" Synthetic casings in polyamide"Appl.. |
|||
Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1, -3 |
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, injection molding, halogen free flame retardant.Information provided by LANXESS. |
|||
Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
Lanxess Durethan® DP 2131/20 H2.0 900051 Nylon 6, 20% Glass Fiber PA 6, injection molding grade, 20% glass fibers, better surface resistance to alcoholic calcium chloride-solution than BKV 20 H2.0, good heat-ageing resistance and weather resistance |
|||
Melting Point | 222 °C | 432 °F | 10 °C/min; ISO 11357-1,-3 |
Lanxess Durethan® DP 2131/20 H3.0 000000 Nylon 6, 20% Glass Fiber PA 6, 20% glass fiber, injection molding, heat-ageing stabilized, weather stabilized, improved surface finishInformation provided by LANXESS. |
|||
Melting Point | 222 °C | 432 °F | 10 °C/min; ISO 11357-1,-3 |
Lanxess Pocan® BF 4232 000000 PBT, 30% Glass Fiber PBT, 30% glass fiber, injection molding, flame retardantInformation provided by LANXESS. |
|||
Melting Point | 222 °C | 432 °F | ISO 11357-1,-3 |
Lanxess Durethan® BM 240 H3.0 000000 Nylon 6, 40% Mineral PA 6, 40% mineral, injection molding, heat-ageing stabilized, low tendency to warp, isotopic properties |
|||
Melting Point | 222 °C | 432 °F | ISO 11357 |
Solvay TECHNYL® C 216 PA6, DRY Description: Unreinforced polyamide PA6, standard nucleation for fast cycling, for injection molding.Available in: Asia PacificProduct Applications: This grade has a high fluidity and good mould rel.. |
|||
Melting Point | 222 °C | 432 °F | ISO 3146-C |
Solvay Technyl® C 218 MT25 V15 25% Mineral, 15% Glass Filled, Heat Stabilized Nylon 6 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Melting Point | 222 °C | 432 °F | ISO 3146-C |
Solvay Technyl® C 218 V50 50% Glass Filled, Heat Stabilized Nylon 6 Information provided by Rhodia; Rhodia has been acquired by Solvay. |
|||
Melting Point | 222 °C | 432 °F | ISO 11357 |
Solvay TECHNYL® C 52G1 V20 PA6, DRY Description: Halogen and Red Phosphorous free fire resistant polyamide PA6 Glass reinforced for injection molding of thin walled partsAvailable in: Asia Pacific, Europe, Latin America and North Amer.. |
|||
Melting Point | 222 °C | 432 °F | ISO 11357 |
Solvay TECHNYLSTARâ„¢ S 216L2 V30 PA6, 30% glass filled, DRY Description: TECHNYLSTAR polyamide reinforced with 30% GF, UV stabilized, for Injection molding. Available in: Europe and North AmericaProduct Applications: TECHNYLSTAR TM S 216L2 V30 BLACK is chara.. |
|||
Melting Point | 222 °C | 432 °F | ISO 11357 |
Solvay TECHNYLSTARâ„¢ SX 216 V50 PA6, 50% glass filled, DRY Description: TECHNYLSTAR Polyamide, reinforced with 50% of glass fiber, characterized by a high fluidity of the melt, for injection molding.Available in: Asia Pacific, Europe and North America Produ.. |
|||
Melting Point | 222 °C | 432 °F | |
Samyang Tribit® 1503S Polybutylene Terephthalate Characteristics:High impactApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll information provided by Samyang |
|||
Melting Point | 222 °C | 432 °F | ISO 11357 |
Suzhou Hipro Polymers Hiprolon® 70 MC HLS G30 Nylon 610, 30% glass fiber filled Hiprolon® 70 MC HLS G30 polyamide 6.10 compound reinforced with 30% chopped glass fiber for injection molding. Features: high heat resistance, dimension stability, impact resistance, good flow ab.. |
|||
Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® BG-15 HM PA6-GF15 Product description: Grilon BG-15 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 15% glass fibers. Grilon BG-15 HM has the following important prop.. |
|||
Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® BG-40 HM PA6-GF40 Product description: Grilon BG-40 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 40% glass fibers. Grilon BG-40 HM has the following important prop.. |
|||
Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® BG-50 HM PA6-GF50 Product description: Grilon BG-50 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 50% glass fibers. Grilon BG-50 HM has the following important prop.. |
|||
Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® BGZ-40 PA6-GF40 Product description: Grilon BGZ-40 is a normal viscosity, heat stabilized and impact modified PA 6 injection molding type with 40% glass fibers. Grilon BGZ-40 has the following important properties:.. |
|||
Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® F 47 NL nat 6028 PA6 Product description: Grilon F 47 NL natural 6028 is a nucleated, high viscosity polyamide 6. This product exhibits the following features: Good gas barrierGood mechanical propertiesGood barrier agai.. |
|||
Melting Point | 222 °C | 432 °F | ASTM D789 |
Adell BR-13 Nylon 6, 15% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® XE 4192 black 9992 PA610-GF30 Information provided by EMS Grivory |
|||
Melting Point | 222 °C | 432 °F | ISO 11357 |
Solvay TECHNYL® 1015CR PA6, DRY Description: Polyamide 6, unfilled, standard for fast injection cycles, for injection molding Available in: Asia Pacific Product Applications: TECHNYL® 1015CR has high fluidity and a good mould re.. |
|||
Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® BGZ-15/2 PA6-GF15 Product description: Grilon BGZ-15/2 is a heat stabilized and impact modified PA6 injection molding grade with 15% glass fibers. Grilon BGZ-15/2 has the following important properties: Good impact s.. |
|||
Melting Point | 222 °C | 432 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® F 50 nat 6368 PA6 Product description: Grilon F 50 natural 6368 is a modified, very high viscous Polyamide 6 for extrusion processes: Very high melt strengthGood chemical resistanceGood gas-barrierGood mechanical pro.. |