Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 125 °C | 257 °F | Compression Molded; ASTM E794 |
NOVA Chemicals Surpass® RMs539-U Octene sMDPE Rotational Molding Film Features: Octene copolymerExceptional low temperature impact propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Stan.. |
|||
Melting Point | 125 °C | 257 °F | |
Mitsui Fybrel® UL 415 Polyolefin Synthetic Pulp, Dry Processes
(discontinued **) Fybrel® (Polyolefin Synthetic Pulp) is a highly fibrillated fiber similar to wood pulp. There are three types available: Fybrel® E and Fybrel® UL, which are both made from polyethylene, and Type .. |
|||
Melting Point | 125 °C | 257 °F | ASTM D3418 |
ExxonMobil LLP8455.24 Rotational Molding Resin
(discontinued **) LL 8450 is a linear low density butene copolymer designed to offer excellent processability, whiteness and fast grinding rate. This resin is ideally suited for applications that require excellent di.. |
|||
Melting Point | 125 °C | 257 °F | Exxon Method |
ExxonMobil Escorene® LL-3001 LLDPE/Hexene Premium Film Resin, Tough, 1.2 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE film resin. Films made from LL-3001 have outstanding tensile and toughness properties. The superior strength properties a.. |
|||
Melting Point | 125 °C | 257 °F | Exxon Method |
ExxonMobil Escorene® LL-3001 LLDPE/Hexene Premium Film Resin, Tough, 0.6 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE film resin. Films made from LL-3001 have outstanding tensile and toughness properties. The superior strength properties a.. |
|||
Melting Point | 125 °C | 257 °F | Exxon Method |
ExxonMobil Escorene® LL-3105 LLDPE/Hexene Premium Film Resin, Tough, 1.2 mil film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3105 have outstanding tensile and toughness properties. The superior strength propert.. |
|||
Melting Point | 125 °C | 257 °F | Petromont |
Petromont 2100 Medium Density Polyethylene Resin Petromont HDPE 2100 is a medium density polyethylene blown film resin produced using the UNIPOL™ Process. This resin is designed specifically for blown film made by co-extrusion. It is commonly use.. |
|||
Melting Point | 125 - 190 °C | 257 - 374 °F | Huntsman/TMA |
Huntsman IROGRAN® A 70 E 4675 Polyester-Based TPU-High Performance Grade Introduction: IROGRAN A 70 E 4675 is a softener free thermoplastic special-polyester-polyurethane for injection molding applications. Additional characteristics of the product are very short cycle t.. |
|||
Melting Point | 125 - 144 °C | 257 - 291 °F | TMA Melt Range |
Huntsman IROGRAN® PS 455-204 TPU-Polyester Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers |
|||
Melting Point | 125 - 129 °C | 257 - 264 °F | Sheath Melt Point; LCL-PR29 |
Intercontinental Polymers 1138 Bicomponent HDPE/PET Fiber Type - 3 Denier X 2.5 Inches 50/50 HDPE Sheath/PET Core. Luster: Semi-Dull. Finish: Hydrophilic.Applications of bicomponent polyester fiber: Absorbent products, hygiene products, non-wovens, filtration, sliver knit, microdeni.. |
|||
Melting Point | 125 - 129 °C | 257 - 264 °F | Sheath Melt Point; LCL-PR29 |
Intercontinental Polymers 1171 Bicomponent HDPE/PET Fiber Type - Denier 1.8 X 1.5 Inches 50/50 HDPE Sheath/PET Core. Luster: Semi-Dull. Finish: Hydrophilic.Applications of bicomponent polyester fiber: Absorbent products, hygiene products, non-wovens, filtration, sliver knit, microdeni.. |
|||
Melting Point | 125 - 135 °C | 257 - 275 °F | |
LG Chemical LUTENE XL8080TR PE Compound Description: LUTENE XL8080TR has excellent electrical properties for medium and high voltage power cable insulation and especially it shows improved water tree resistance and has thermal aging prope.. |
|||
Melting Point | 125 °C | 257 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ M3504DXP Octene (C8) Rotational Molding Resin Natural base resin available in powder formKey Characteristics:Excellent ESCRExcellent impact resistanceLow warpageFair processingTypical Applications: Chemical storage tanks, diesel tanks, spray t.. |
|||
Melting Point | 125 °C | 257 °F | Melting point via DSC/ASTM D3418 |
DuPont Bynel® 4104 Anhydride-Modified LLDPE Adhesive Resin Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Melting Point | 125 °C | 257 °F | Melting point via DSC/ASTM D3418 |
DuPont Bynel® 4105 Anhydride-Modified LLDPE Adhesive Resin Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Melting Point | 125 °C | 257 °F | Kofler |
Lubrizol ESTANE® 58630 Ether Based Thermoplastic Polyurethane Features: Good physical properties, hydrolysis resistance, low temperature performance and abrasion along with wide processing window for extrusion and low surface tack.Uses: Blown and flat die/cast.. |
|||
Melting Point | 125 - 129 °C | 257 - 264 °F | crystalline; DSC |
Total 3802 YCF MDPE pipe grade FINATHENE® 3802 Y CF is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Y CF is a yellow cadmi.. |
|||
Melting Point | 125 °C | 257 °F | ASTM D3417 |
Total HDPE 7194 High Density Polyethylene, Specialty Extrusion Resin Medium molecular weightNarrow molecular weight distributionDesigned for high speed orientationUSP Class VI compliantApplications:MonofilamentSlit tapeWoven and knitted fabricsSpecialty filmsInformat.. |
|||
Melting Point | 125 °C | 257 °F | ASTM D3417 |
Total HDPE 7195 High Density Polyethylene, Specialty Extrusion Resin Characteristics:Medium molecular weightNarrow molecular weight distributionDesigned for high speed orientationApplications:MonofilamentSlit tapeWoven and knitted fabricsSpecialty filmsInformation pr.. |
|||
Melting Point | 125 - 130 °C | 257 - 266 °F | DSC |
EMS-Griltech Griltex® 6E Copolyester Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melting Point | 125 °C | 257 °F | ASTM D3418, ISO 3146 |
DuPont™ Bynel® 41E755 Anhydride Modified LLDPE BYNEL® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Melting Point | 125 °C | 257 °F | ASTM D3418 |
ExxonMobil LLP8360.29 Rotational Molding Resin Product Description: LL 8360 is a linear low density hexene copolymer designed to offer excellent processability along with outstanding dimensional control and low warpage. This resin is ideally sui.. |
|||
Melting Point | 125 °C | 257 °F | Dow Method (DSC) |
Dow DFDC-7525 NT High Density Polyethylene Resin DOW DFDC-7525 NT is produced using UNIPOL™ process technology. It is intended for use in thin wall drip tape and micro-irrigation tube, hose and tube, and profile extrusion applications. Informati.. |
|||
Melting Point | 125 °C | 257 °F | Dow Method (DSC) |
Dow DOWLEX™ 2036G Linear Low Density Polyethylene Improved thermal stability for high stiffness film applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Melting Point | 125 °C | 257 °F | Dow Method (DSC) |
Dow ASPUN™ 6811A Linear Low-Density Polyethylene (LLDPE) ASPUN™ 6811A Fiber Grade Resin: Suggested Optimum Process: Spun Bond Typical Application: Non-woven FabricsInformation provided by Dow |
|||
Melting Point | 125 °C | 257 °F | ASTM-D3418 |
Braskem RA34U3 LLDPE Rotomolding Polyethylene The resin RA34U3 is a linear low-density polyethylene, 1-butene based, with a good balance of processability, environmental stress cracking resistance, and impact strength. It contains long term UV6.. |
|||
Melting Point | 125 °C | 257 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LL 3201.22 Premium High Strength Film Resin
(discontinued **) LL 3201 resins are hexene copolymer LLDPE film resins. Films produced from these resins have excellent tensile, toughness and stiffness properties. These strength properties, along with good drawdow.. |
|||
Melting Point | 125 °C | 257 °F | ASTM D2117 |
SCG Chemicals EL-Lene™ M50 Octene (C8) Rotational Molding Resin Color compound resin available in pellet / powder formKey Characteristics:Excellent ESCRExcellent impact resistanceLow warpageFair processingTypical Applications: Chemical storage tanks, diesel tan.. |
|||
Melting Point | 125 °C | 257 °F | Exxon Method |
ExxonMobil Escorene® LL-8302 LMDPE Rotational Molding Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.LL-8300 series are linear medium density polyethylene resins that provide outstanding environmental stress crack resistance. LL-8302 is the base re.. |