Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total HDPE 7195 High Density Polyethylene, Specialty Extrusion Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Extruded
Manufacturer Total Atofina
Trade Name HDPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total HDPE 7195 High Density Polyethylene, Specialty Extrusion Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics:Medium molecular weightNarrow molecular weight distributionDesigned for high speed orientationApplications:MonofilamentSlit tapeWoven and knitted fabricsSpecialty filmsInformation provided by Total Petrochemicals.
Physical Properties Metric English Comments
Density 0.946 g/cc
0.0342 lb/in³
ASTM D792
Melt Flow 0.55 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.55 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
1.9 g/10 min

@Load 5.00 kg,
Temperature 190 °C
1.9 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.1 MPa
3200 psi
ASTM D638
Elongation at Break >= 500 %
>= 500 %
ASTM D638
Flexural Modulus 0.793 GPa
115 ksi
ASTM D790
2% Secant Modulus 0.689 GPa
100 ksi
ASTM D638
Thermal Properties Metric English Comments
Melting Point 125 °C
257 °F
ASTM D3417
Descriptive Properties Value Comments
Process Extrusion
Region US & Canada
Bamberger Polymers Distribution