Thermal Properties Metric English Comments
Melting Point 74.0 °C
165 °F
Internal Method
Polimeri Europa Greenflex® ML 60 Ethylene Vinyl Acetate Copolymer - Injection Molding, Compounding & Extrusion
Greenflex ML 60 is an ethylene vinyl acetate copolymer (EVA) for injection molding, compounding and extrusion. Items produced with Greenflex ML 60 show very high elasticity.Main Applications: Gree..
Melting Point 74.0 °C
165 °F
Exxon Method
ExxonMobil Optema® TC-113 Ethylene Methyl Acrylate for Compounding  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.23.5% Methyl Acrylate. An Ethylene Methyl Acrylate copolymer which can be used as an impact modifier or compatibilizer in polymer compounds. It ca..
Melting Point 74.0 - 84.0 °C
165 - 183 °F
Fine Organics FINALUX GH 41 Lubricant Additive
Applications: Internal lubricant for rigid PVC injection molded fittings, calendered, blown films/sheets, PVC bottles and other Sn-mercaptide stabilized rigid PVC products. Excellent synergistic co..
Melting Point 74.0 °C
165 °F
Melting point via DSC/ASTM D3418
DuPont Bynel® 3860 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
Bynel® Series 3800 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Melting Point 74.0 °C
165 °F
Freezing Point, DSC; ASTM D3418
DuPont Bynel® 39E660 Adhesive Resin
Bynel® Series 3900 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Melting Point 74.0 °C
165 °F
Melting point via DSC/ASTM D3418
DuPont Bynel® E418 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
Bynel® Series 3800 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Melting Point 74.0 - 92.0 °C
165 - 198 °F
ASTM D3418(DSC)
DuPont Nucrel® 925 Ethylene-Methacrylic Acid Copolymer Resin
Nucrel® 925 is a tough, lightweight, easily processed ethylene copolymer resin. This resin is inherently flexible without the need for plasticizers. The resin can be pigmented, UV-stabilized for ..
Melting Point 74.0 °C
165 °F
Freezing Point; ASTM D3418
DuPont Trancend™ Extrusion Coating Sealant
DuPont™ Trancend™ is an ethylene acrylic acid ionomer, expressly designed for extrusion coating, using a new generation of manufacturing technology. This new technology has allowed DuPont to produ..
Melting Point 74.0 °C
165 °F
DSC; ASTM D3418
Westlake Tymax™ GT7058 Anhydride Modified Acrylate Copolymer
Westlake GT7058 is an anhydride modified acrylate copolymer designed for blown film extrusion that contains no slip and no antiblock additives. This resin is designed to function as a coextruded tie..
Melting Point 74.0 °C
165 °F
Upon Melting via DSC/ASTM D3418
DuPont Bynel® 1123 Modified EVA Adhesive Resin
Bynel® Series 1100 resins are modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylen..
Melting Point 74.0 °C
165 °F
ASTM D3417- ISO 3146
DuPont Elvax® 350 Ethylene Vinyl Acetate
DuPont™ Elvax® 350 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Addition: antiblock Applications:Elvax® 350 resins can be used for the following applications: ..
Melting Point 73.9 °C
165 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil Escorene® AD2528 Adhesive Application Resin
Escorene Ultra AD 2528 is a very high flow rate, 27.6% Vinyl Acetate, copolymer, which is useful in formulating hot melt adhesives.Availability: Latin America, North America and South America Additi..
Melting Point 73.9 °C
165 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil Escorene® UL 7765 Adhesive Application Resin
Escorene Ultra UL 7765 is a high viscosity, 26.2% vinyl acetate copolymer that has very good flexibility and low temperature toughness. It has good compatibility with both hydrocarbon and natural t..
Melting Point 74.0 °C
165 °F
Freezing Point; ASTM D3418, ISO 3146
DuPont™ Bynel® 21E787 Anhydride Modified Ethylene Acrylate
BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available i..
Melting Point 74.0 °C
165 °F
ASTM D3418, ISO 3146
DuPont™ Elvax® 3175LGA Ethylene Vinyl Acetate
DuPont™ Elvax® 3175LGA is an extrudable ethylene-vinyl acetate copolymer resin containing low gel material available in pellet form for use in conventional extrusion equipment designed to process ..
Melting Point 74.0 °C
165 °F
by DSC; ASTM D3418
Westlake EMAC® SP2261 23% Ethylene-Methyl Acrylate Copolymer
Westlake EMAC® SP2261 is a 23% EMA copolymer containing antiblock. This resin is designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal tempe..
Melting Point 74.0 °C
165 °F
DSC; ASTM D3417- ISO 3146
DuPont Elvax® 240 Ethylene Vinyl Acetate  (discontinued **)
DuPont™ Elvax® 240 is an ethylene-vinyl acetate copolymer resin for use in industrial applications. Applications:Elvax® 240 resins can be used for the following applications: adhesives, sealants,..