Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 74.0 - 84.0 °C | 165 - 183 °F | |
Fine Organics FINALUX GH 41 Lubricant Additive Applications: Internal lubricant for rigid PVC injection molded fittings, calendered, blown films/sheets, PVC bottles and other Sn-mercaptide stabilized rigid PVC products. Excellent synergistic co.. |
|||
Melting Point | 80.0 - 84.0 °C | 176 - 183 °F | MQSA 70 A |
Lubrizol Advanced Materials Pearlbond® ECO D590 Thermoplastic Polyurethane Pearlbond™ ECO D590 is a linear, aromatic bio-polyurethane based on specialty polyol from renewable sources, supplied in form of white spherical granules, with an extremely high crystallization.. |