Polymer Property : Melting Point = 84.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 74.0 - 84.0 °C
165 - 183 °F
Fine Organics FINALUX GH 41 Lubricant Additive
Applications: Internal lubricant for rigid PVC injection molded fittings, calendered, blown films/sheets, PVC bottles and other Sn-mercaptide stabilized rigid PVC products. Excellent synergistic co..
Melting Point 80.0 - 84.0 °C
176 - 183 °F
MQSA 70 A
Lubrizol Advanced Materials Pearlbond® ECO D590 Thermoplastic Polyurethane
Pearlbondâ„¢ ECO D590 is a linear, aromatic bio-polyurethane based on specialty polyol from renewable sources, supplied in form of white spherical granules, with an extremely high crystallization..