Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 164 - 168 °C | 327 - 334 °F | ISO 3146 |
Borealis Bormod™ HC905TF Polypropylene Homopolymer for Thermoforming Bormod HC905TF is a low melt flow rate polypropylene homopolymer intended for thermoformed packaging applications. This homopolymer is produced using the Borealis Controlled Crystallinity Polypropy.. |
|||
Melting Point | 164 - 168 °C | 327 - 334 °F | ISO 1218 Method A; DIN 53736 |
Zell-Metall Engineering Plastics Zellamid 900 (POM-C) Zellamid® 900 is the registered trademark of Zell-Metalls high molecular weight Acetal resin.Acetal (POM) is noted for its high mechanical strength, heat resistance and good antifriction .. |
|||
Melting Point | 164 - 168 °C | 327 - 334 °F | ISO 1218 Method A; DIN 53736 |
Zell-Metall Engineering Plastics Zellamid 900 (POM-C) at 50% RH Zellamid® 900 is the registered trademark of Zell-Metalls high molecular weight Acetal resin.Acetal (POM) is noted for its high mechanical strength, heat resistance and good antifriction prope.. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene H 210 G20 Polypropylene Homopolymer Glass bead reinforced, improved stiffness and dimensional stabilityInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene H 290 M20F Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene H 490 M10S Flame Retardant Polypropylene Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene H 490 M20F Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene H 530 N30 Polypropylene Homopolymer Good surface appearanceInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene H 560 Polypropylene Homopolymer High heat resistance, detergent stabilized, anti-yellowingInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene H 590 RM20F Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogens, impact resistantInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene J 310 Polypropylene Copolymer UnreinforcedInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene J 370 Polypropylene Copolymer High impact strength, high elongation at breakInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene J 420 K24 Polypropylene Copolymer High densityInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene J 520 M40 Polypropylene Copolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene J 522 K20 Polypropylene Copolymer High densityInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene J 522 M20 Polypropylene Copolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene J 522 N30 Polypropylene Copolymer Mineral reinforced, improved scratch resistanceInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene J 690 RM20F Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogens, impact resistantInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene PMD 50213 Polypropylene Copolymer Mineral reinforced, improved scratch resistanceInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene PMD 50258 Polypropylene Copolymer For electroplatingInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene J 220 M40 Polypropylene Copolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene J 290 M20F Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene J 520 T30 Polypropylene Copolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene PMD 50284 Polypropylene Copolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene PMD 50306 Polypropylene Copolymer Mineral reinforced, improved scratch resistanceInformation provided by Addiplast. |
|||
Melting Point | 162 - 168 °C | 324 - 334 °F | ASTM D3418 |
Solvay Specialty Polymers Solef® 9007 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 9007 PVDF homopolymer has low viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers. |
|||
Melting Point | 162 - 168 °C | 324 - 334 °F | ASTM D3418 |
Solvay Specialty Polymers Solef® 9009 Polyvinylidene Fluoride (PVDF)
(discontinued **) Solef® 9009 PVDF homopolymer has low/medium viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene PMD 50291 Flame Retardant Polypropylene Flame retardant, high rigidityInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene H 552 Y7 Polypropylene Homopolymer Good surface appearance, high temperature resistanceInformation provided by Addiplast. |
|||
Melting Point | 165 - 168 °C | 329 - 334 °F | ISO 3146/C2 |
Addiplast Addilene PMD 50203 Flame Retardant Polypropylene Flame retardant, unreinforced, with halogensInformation provided by Addiplast. |