Material Notes:
Mineral reinforced, improved scratch resistanceInformation provided by Addiplast.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ISO 1183/A
Melt Flow 10 g/10 min
10 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
ISO 868
Tensile Strength at Break 15.0 MPa
2180 psi
ISO R 527
Tensile Strength, Yield 20.0 MPa
2900 psi
ISO R 527
Elongation at Yield 20 %
20 %
ISO R 527
Modulus of Elasticity 2.00 GPa
290 ksi
ISO 178
Izod Impact, Notched (ISO) 14.0 kJ/m²
6.66 ft-lb/in²
ISO 180/1A
Charpy Impact Unnotched NB
NB
ISO 179/IeU
Charpy Impact, Notched 1.50 J/cm²
7.14 ft-lb/in²
ISO 179/IeA
Thermal Properties Metric English Comments
Melting Point 165 - 168 °C
329 - 334 °F
ISO 3146/C2
Deflection Temperature at 1.8 MPa (264 psi) 58.0 °C
136 °F
ISO 75-2/AF
Vicat Softening Point 146 °C
295 °F
ISO 306/A50
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+13 ohm-cm
>= 1.00e+13 ohm-cm
CEI 60093
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
CEI 60093
Comparative Tracking Index >= 600 V
>= 600 V
CEI 60112/Solution A