Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melting Point = 172 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 166 - 172 °C
331 - 342 °F
Indium Corp. Indalloy 234 Bismuth-Lead-Tin Solder Alloy
Information Provided by Indium Corporation
Melting Point 160 - 172 °C
320 - 342 °F
Hong Kun Group Aluminum-N-nitroso-N-phenylhydroxyamine Additive
CAS No. 15305-07-4All information provided by Hongkun Group
Melting Point 164 - 172 °C
327 - 342 °F
ASTM D3418
Shanghai Ofluorine T-2 PVDF for Powder Coatings
Description: T-2 PVDF belong to thermoplastic fluorocarbon resin, which has high melt flow rate, low melt viscosity. T-2 PVDF has characteristic of chemical resistance, heat resistance, high mechani..
Melting Point 114 - 172 °C
237 - 342 °F
Dow Method (DSC)
Dow Saran® 506 Polymer
Saran™ 506 Polymer is designed as an ignition resistant adhesive bonding agent. Saran™ 506 is a vinylidene chloride copolymer supplied as a white, micronized powder. It is unaffected by humidity..
Melting Point 165 - 172 °C
329 - 342 °F
Arkema Group KYNAR® 1000 HD Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Melting Point 165 - 172 °C
329 - 342 °F
Arkema Group KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Low melt shrinkage, graphite powder filled. High stability in harsh thermal, chemical and ultraviolet environments. High toug..
Melting Point 165 - 172 °C
329 - 342 °F
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Melting Point 165 - 172 °C
329 - 342 °F
Arkema Group KYNAR® 740 Black/Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purityAppli..
Melting Point 165 - 172 °C
329 - 342 °F
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Melting Point 165 - 172 °C
329 - 342 °F
Arkema Group KYNAR® 740-02 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mecha..
Melting Point 165 - 172 °C
329 - 342 °F
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Melting Point 165 - 172 °C
329 - 342 °F
Arkema Group KYNAR® 6000 HD Polyvinylidene Fluoride - Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Melting Point 165 - 172 °C
329 - 342 °F
Arkema Group KYNAR® 711 Polyvinylidene Fluoride Powder
Characteristics: White, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistan..
Melting Point 165 - 172 °C
329 - 342 °F
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Melting Point 165 - 172 °C
329 - 342 °F
Arkema Group KYNAR® 721 Polyvinylidene Fluoride Powder
Characteristics: White, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistan..
Melting Point 165 - 172 °C
329 - 342 °F
Arkema Group KYNAR® 741 Polyvinylidene Fluoride Powder
Characteristics: White, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistan..
Melting Point 165 - 172 °C
329 - 342 °F
Arkema Group KYNAR® 9000 HD Polyvinylidene Fluoride - Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Melting Point 158 - 172 °C
316 - 342 °F
Arkema Group KYNAR® HSV Polyvinylidene Fluoride Powder
Characteristics: White, non-hygroscopic powder.Applications: Membrane, Lithium ion battery applicationsInformation provided by Arkema Inc.
Melting Point 169 - 172 °C
336 - 342 °F
BASF 2,3,5-Trimethylhydroquinone
Formula: C9H12O2CAS: 700-13-0Description: TMHQ is a colorless fine crystalline powder. It is insoluble in water, soluble in methanol, ethanol, diethyl ether, and acetone.Synonyms: TMHQ, TMHApplicat..
Melting Point 165 - 172 °C
329 - 342 °F
Arkema Group KYNAR® 761 Polyvinylidene Fluoride Powder
Characteristics: White, non-hygroscopic powder. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistan..
Copyright © lookpolymers.com All Rights Reserved