Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 250 - 258 °C | 482 - 496 °F | DSC @ 15°C / min; ASTM D3418 |
Ovation Polymers RIGITRON 30530 GF Polyester, 30% Glass Reinforced Polyester – 30 % Glass Fiber Reinforced PET. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM standards. Va.. |
|||
Melting Point | 250 - 258 °C | 482 - 496 °F | DSC @ 15°C / min; ASTM D3418 |
Ovation Polymers RIGITRON 30545 GF Polyester, 45% Glass Reinforced Polyester – 45% Glass Fiber Reinforced PET. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM standards. Var.. |
|||
Melting Point | 252 - 258 °C | 486 - 496 °F | DSC |
Iran Petrochemical (PCC) TG 621 Polyethylene Terephthalate Polyethylene Terephthalate fiber grade chips, semi dullApplications: staple fiber, spunbond, meltblown nonwovensInformation provided by Iran Petrochemical Commercial Co. |
|||
Melting Point | 252 - 258 °C | 486 - 496 °F | DSC |
Iran Petrochemical (PCC) TG 641 Polyethylene Terephthalate Polyethylene Terephthalate fiber grade chips, semi dullApplications: staple fiber, textile filament, spunbond, meltblown nonwovensInformation provided by Iran Petrochemical Commercial Co. |
|||
Melting Point | 252 - 258 °C | 486 - 496 °F | DSC |
Iran Petrochemical (PCC) TG 641 Super Bright Polyethylene Terephthalate Polyethylene Terephthalate fiber grade chips, super brightApplications: staple fiber, textile filament, spunbond, meltblown nonwovensInformation provided by Iran Petrochemical Commercial Co. |
|||
Melting Point | 252 - 258 °C | 486 - 496 °F | DSC |
Iran Petrochemical (PCC) TG 645 Super Bright Polyethylene Terephthalate Polyethylene Terephthalate fiber grade chips, super brightInformation provided by Iran Petrochemical Commercial Co. |
|||
Melting Point | 250 - 258 °C | 482 - 496 °F | |
Isoflon Polyester film Polyethylene terephthalate film is a flexible film with high mechanical resistance. An excellent insulator, it preserves all its properties in a wide range of temperatures (-70°C to +150°C). .. |
|||
Melting Point | 252 - 258 °C | 486 - 496 °F | DSC |
Iran Petrochemical (PCC) TG 645 Polyethylene Terephthalate Polyethylene Terephthalate fiber grade chipsInformation provided by Iran Petrochemical Commercial Co. |
|||
Melting Point | 252 - 258 °C | 486 - 496 °F | DSC |
Iran Petrochemical (PCC) TG 732 Polyethylene Terephthalate Polyethylene Terephthalate fiber grade chipsInformation provided by Iran Petrochemical Commercial Co. |