Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 147 °C | 297 °F | Flow temperature, ASTM D569-59 |
Rotuba 870 Ethyl Cellulose Data provided by the manufacturer. |
|||
Melting Point | 147 °C | 297 °F | |
Honeywell Spectra® 1000 Fiber Spectra® fiber 1000, the second in a series of Spectra® fibers, was developed to meet customers’ needs for increased performance. It is available in a multitude of deniers for use in a wi.. |
|||
Melting Point | 147 °C | 297 °F | |
Honeywell Spectra® 900 Fiber Spectra® fiber 900 was the first commercially available extended-chain, high-strength polyethylene fiber and the first in a series of Spectra® fibers. Spectra® fiber has one of the highest .. |
|||
Melting Point | 147 - 151 °C | 297 - 304 °F | |
M Chemical GUARD DOG™ UV1577 Light Absorber, Triazene Derivative GUARD DOG™ UV1577 UV absorber is a low volatile Triazine based UV absorber which is highly effective in polymers that are processed at high temperature (decomposition temperature > 350°C).Ap.. |
|||
Melting Point | 147 °C | 297 °F | |
Hyosung Topilene R500F PP R500F Block CopolymerApplications: Retort CPPCharacteristics:Excellent impact strengthFish eye freeHeat resistanceGood clarityInformation provided by Hyosung Corporation |
|||
Melting Point | 147 °C | 297 °F | |
Hyosung Topilene R500S PP R500S Block CopolymerApplications: Retort CPPCharacteristics:Excellent impact strengthFish eye freeHeat resistanceGood clarityInformation provided by Hyosung Corporation |
|||
Melting Point | 147 °C | 297 °F | TMA; MCI Method |
Mitsui APELâ„¢ APL5014DP Cyclo Olefin Copolymer (COC) This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt proces.. |
|||
Melting Point | 147 °C | 297 °F | ISO 3146 |
Total PPR 10222 Random Copolymer Polypropylene, Injection Molding Total Petrochemicals PPR 10222 is a nucleated and antistatic random copolymer polypropylene with a melt flow index of 40 g/10min for the injection molding of articles with high transparency and exce.. |
|||
Melting Point | 147 °C | 297 °F | ISO 3146 |
Total PPR 10232 Random Copolymer Polypropylene, Injection Molding Total Petrochemicals PPR 10232 is a nucleated and antistatic random copolymer polypropylene with a melt flow index of 40 g/10min for the injection molding of articles with high transparency and exce.. |
|||
Melting Point | 147 °C | 297 °F | ASTM D3428 |
CRG Industries Essemplex AF34 Thermoplastic Shape Memory Polymer Resin Essemplex is a melt-processible shape memory polymer (SMP) resin. Its unique properties offer versatile design options for reconfiable and customizable products. Essemplex is compatible with current.. |
|||
Melting Point | 147 °C | 297 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Hytrel® 21UV Polyester Elastomer TPC-ET
(Unverified Data**) Polyester Elastomer Concentrate Developed for Enhancing UV ResistanceInformation provided by DuPont Performance Polymers |
|||
Melting Point | 147 °C | 297 °F | ISO 11357 |
Arkema Group Pebax® MX 1205 SA 01 MED Polyether Block Amide (PEBA) Polyether block amide PEBAX® MX 1205 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to mee.. |
|||
Melting Point | 147 °C | 297 °F | ISO 11357 |
Arkema Group Pebax® MX 1205 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® MX 1205 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arke.. |
|||
Melting Point | 147 °C | 297 °F | 10°C/min |
Arkema Group Pebax® MX 1205 SN 01 Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE (PEBA) hardness 40 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness.. |
|||
Melting Point | 147 - 165 °C | 297 - 329 °F | Average value: 160 °C Grade Count:11 |
Overview of materials for Polypropylene, Sheet/Thermoforming Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Sheet/Thermoforming Grade". Each property range of values reported is minimum and maximum.. |
|||
Melting Point | 147 °C | 297 °F | ASTM D3418 |
Arkema Group Pebax® MX 1205 Polyether Block Amide (PEBA) Typical application: Impact modifierInformation provided by Arkema Group |
|||
Melting Point | 147 °C | 297 °F | (Dry) |
Arkema Group Pebax® MX 1205 SN 01 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) hardness 40 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness.. |
|||
Melting Point | 147 °C | 297 °F | ISO 11357 |
Arkema Group Pebax® MX 1205 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® MX 1205 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information prov.. |