Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 150 °C | 302 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVALEN PC 51 T 20 Polypropylene Copolymer, 20% Micronized Talc FeaturesModified copolymer PP for injection moulding with the content of 20% micronized, floated, chemically modified talc. General application in all industry branches - packing material, garden f.. |
|||
Melting Point | 150 °C | 302 °F | |
Plastcom SLOVALEN PC 51 T 25 PP, 25% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 25% microground, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitu.. |
|||
Melting Point | 150 °C | 302 °F | |
Plastcom SLOVALEN PC 53 T 25 PP, 25% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 25% microground, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitu.. |
|||
Melting Point | 150 °C | 302 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVALEN PC 78 FRD 3 Polypropylene Copolymer, Halogen Flame Retardant FeaturesDetermined for environment where contact with water is possible because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machine.. |
|||
Melting Point | 150 °C | 302 °F | |
Plastcom SLOVALEN PC 81 T 15 PP, 15% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 15% micronized, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitur.. |
|||
Melting Point | 150 °C | 302 °F | |
Plastcom SLOVALEN PC 81 T 30 PP, 30% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 30% microground, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitu.. |
|||
Melting Point | 150 °C | 302 °F | |
Plastcom SLOVALEN PC 82 T 30 PP, 30% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 30% micronized, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitur.. |
|||
Melting Point | 150 °C | 302 °F | |
Plastcom SLOVALEN PC 91 C 20 PP, 20% mineral filling FeaturesModified copolymer PP for injection moulding with the contenct of 20% microground, chemically modified talc. Increased strength, rigidity and thermal application up to 100°C depending on th.. |
|||
Melting Point | 150 °C | 302 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVALEN PH 51 C 40 Polypropylene Homopolymer and Copolymer, 40% Micronized Talc FeaturesModified homopolymer and copolymer PP for injection moulding with the content of 40% micronized, chemically modified talc. Increased strength, rigidity and thermal application up to 130°C... |
|||
Melting Point | 150 °C | 302 °F | Flow temperature, ASTM D569-59 |
Rotuba 855, Slow Burning Ethyl Cellulose Data provided by the manufacturer. |
|||
Melting Point | 150 °C | 302 °F | DSC second heating; ASTM D3418 |
Reliance Industries Repol R019MZ Polypropylene REPOL Polypropylene R019MZ is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Melting Point | 150 °C | 302 °F | DSC second heating; ASTM D3418 |
Reliance Industries Repol R110MK Polypropylene REPOL Polypropylene R110MK is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Melting Point | 150 °C | 302 °F | DSC second heating; ASTM D3418 |
Reliance Industries Repol R120MK Polypropylene REPOL Polypropylene R120MK is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Melting Point | 150 °C | 302 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVALEN PC 53 N Polypropylene Copolymer, UV Stabilization FeaturesModified copolymer PP for injection moulding, with the ability of modeling the melt flow rate within the interval 5 - 20 g/10 min. Can be used for simple small as well as for large complica.. |
|||
Melting Point | 150 - 182 °C | 302 - 360 °F | Average value: 159 °C Grade Count:19 |
Overview of materials for Polypropylene with 30% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are.. |
|||
Melting Point | 150 - 170 °C | 302 - 338 °F | ISO 3146-C |
FKuR Kunststoff Bio-Flex® F 6611 Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Melting Point | 150 - 170 °C | 302 - 338 °F | ISO 3146-C |
FKuR Kunststoff Bio-Flex® S 9533 Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Melting Point | 150 - 160 °C | 302 - 320 °F | ISO 3146-C |
FKuR Kunststoff Fibrolon® F 8530 Biodegradable Wood-Plastic Compound, Fiber Reinforced FIBROLON® are fiber reinforced compounds. Depending on specific customer requirements either a biodegradable polymer or a polyolefin can be used as the polymeric matrix. With the brand name of F.. |
|||
Melting Point | 150 - 350 °C | 302 - 662 °F | |
Johnson Matthey JM No1S Soft Solder Flux A highly active liquid flux recommended for use on Stainless and carbon steels. Generally used with the Silver/Tin alloys such as JM P40 and JM P5. Residues are corrosive and should be removed aft.. |
|||
Melting Point | 150 - 300 °C | 302 - 572 °F | |
Johnson Matthey JM No2S Soft Solder Flux A liquid non-corrosive flux for use on copper and brass. The residues are water soluble and non-corrosive, however it is recommended they are removed to prevent any possibility of contamination aft.. |
|||
Melting Point | 150 °C | 302 °F | DSC; ISO 3146 |
Borealis Bormed™ RD804CF Polypropylene Random Copolymer Bormed™ RD804CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications Bormed™ RD804CF is recommended for packaging for med.. |
|||
Melting Point | 150 °C | 302 °F | DSC |
Total PPH M3661 Metallocene Isostatic Polypropylene Polymer, Cast Film Extrusion TOTAL Petrochemicals Polypropylene M3661 is an isostatic form of homopolymer made via TOTAL proprietary metallocene catalyst technologyRecommended Applications. M3661 is a medium molecular weight m.. |
|||
Melting Point | 150 °C | 302 °F | Kofler |
Lubrizol Estane® MVT 70AT3 Thermoplastic Polyurethane, Moisture Vapor Transmission Type: Estane® MVT 70AT3 is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: High moisture vapor transmission with low water swell. Excellent low temperature properties and el.. |
|||
Melting Point | 150 °C | 302 °F | 10°C/min; ISO 11357-1/-3 |
DuPont Performance Polymers Hytrel® PC945 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer Developed for the Healthcare IndustryInformation provided by DuPont Performance Polymers |
|||
Melting Point | 150 °C | 302 °F | |
BASF Novolen® 3248 TC Polypropylene Easy-flowing grade containing nucleating and antistatic agents for transparent injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Melting Point | 150 °C | 302 °F | |
Plastcom SLOVALEN PC 91 T 30 PP, 30% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 30% microground, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitu.. |
|||
Melting Point | 150 °C | 302 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVALEN PH 81 C 40 Polypropylene Homopolymer and Copolymer, 40% Micronized Talc FeaturesModified homopolymer and copolymer PP for injection moulding with the content of 40% micronized, chemically modified talc. Increased strength, rigidity and thermal application up to 130°C... |
|||
Melting Point | 150 - 170 °C | 302 - 338 °F | Average value: 164 °C Grade Count:14 |
Overview of materials for Polypropylene Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Melting Point | 150 - 300 °C | 302 - 572 °F | |
Johnson Matthey JM R-Core Soft Solder Flux A "rosin" type core generally used for joining copper and brass. Residues are non-corrosive.Information provided by Johnson Matthey. |
|||
Melting Point | 150 °C | 302 °F | |
Plastcom SLOVALEN PC 92 T 40 PP, 40% mineral filling FeaturesModified homopolymer and copolymer PP for injection moulding with the contenct of 40% microground, chemically modified talc. Increased strength, rigidity and thermal application up to 100°C.. |