Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 151 °C | 304 °F | Flow temperature, ASTM D569-59 |
Rotuba 860MH 686.4 Ethyl Cellulose Data provided by the manufacturer. |
|||
Melting Point | 151 °C | 304 °F | DSC |
Silon Tabond 5007 Adhesive Resin Tabond 5007 is a chemically modified Polypropylene. Its functional groups improve considerably the bonding between polar polymers, metals and glass.Characteristics: • Strong adhesion to aminosi.. |
|||
Melting Point | 151 °C | 304 °F | ISO 3146 |
Total Lumicene® MR 2001 Polypropylene, Metallocene Polypropylene ATOFINA Polypropylene MR 2001 is a metallocene polypropylene, and is characterized by high fluidity for high speed spinning on spun laid non-woven lines where spun filaments are produced to form a w.. |
|||
Melting Point | 151 °C | 304 °F | ISO 3146 |
Total Lumicene® MR 2002 Polypropylene, Metallocene Polypropylene ATOFINA Polypropylene MR 2002 is a metallocene polypropylene, and is characterized by high fluidity for high speed spinning on spun laid non-woven lines where spun filaments are produced to form a w.. |
|||
Melting Point | 151 °C | 304 °F | DSC |
Total PPH M3766 Metallocene Isostatic Polypropylene Polymer, Fiber Grade M3766 is an isostatic form of polypropylene made via TOTAL proprietary technology.Recommended Applications. M3766 is recommended for melt spun and spun bound fiber applications. However, due to it.. |
|||
Melting Point | 151 °C | 304 °F | DSC |
Total PPH M3865 Metallocene Isostatic Propylene Polymer, Fiber Grade M3865 is an isostatic form of polypropylene made via ATOFINA proprietary technology.Recommended Applications. M3865 is recommended for melt spun and spunbond fiber applications. However, due to it.. |
|||
Melting Point | <= 151 °C | <= 304 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escorene™ UL 7740 Ethylene Vinyl Acetate Copolymer Availability: Latin America, North America and South America Additive: Antiblock: NoSlip: NoThermal Stabilizer: Yes Applications:Adhesives and SealantsIndustrial SealantsHot Melt AdhesivesWax Blends.. |
|||
Melting Point | 151 - 155 °C | 304 - 311 °F | |
Arkema Group KYNAR® LBG2 Polyvinylidene Fluoride Powder Characteristics: White, non-hygroscopic powder.Applications: Membrane, Lithium ion battery applicationsInformation provided by Arkema Inc. |
|||
Melting Point | 151 °C | 304 °F | DSC |
Arkema Group OREVAC® PPC Grafted Maleic Anhydride Polypropylene OREVAC PPC is a grafted maleic anhydride polypropylene used in the manufacturing of multilayer oxygen barrier tube. OREVAC PPC is mainly used in multi-layer tube to have good adhesion between PP, PA.. |