Material Notes:
OREVAC PPC is a grafted maleic anhydride polypropylene used in the manufacturing of multilayer oxygen barrier tube. OREVAC PPC is mainly used in multi-layer tube to have good adhesion between PP, PA and EVOH. OREVAC PPC combined with SOARNOL®from NIPPON GOSHEI provides very good oxygen barrier. These tubes are used in plumbing, sanitary, heating floor and also industrial applications.Information provided by Arkema Group
Physical Properties Metric English Comments
Density 0.890 g/cc

@Temperature 23.0 °C
0.0322 lb/in³

@Temperature 73.4 °F
ISO 1183
Melt Index of Compound 2.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 35.0 MPa
5080 psi
ASTM D638
Tensile Strength, Yield 20.0 MPa
2900 psi
ISO R 527
Elongation at Break 550 %
550 %
ASTM D638
Flexural Modulus 0.580 GPa
84.1 ksi
ASTM D638
Thermal Properties Metric English Comments
Melting Point 151 °C
304 °F
DSC
Vicat Softening Point 122 °C

@Load 0.999 kg
252 °F

@Load 2.20 lb
ISO 306
Processing Properties Metric English Comments
Zone 1 170 - 190 °C
338 - 374 °F
Zone 2 180 - 200 °C
356 - 392 °F
Zone 3 190 - 210 °C
374 - 410 °F
Zone 4 200 - 220 °C
392 - 428 °F
Die Temperature 220 - 240 °C
428 - 464 °F