Rotuba 860MH 686.4 Ethyl Cellulose

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Cellulosic , Ethyl Cellulose, Molded
Manufacturer Rotuba
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Rotuba 860MH 686.4 Ethyl Cellulose.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
ASTM D792-60T
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108
108
ASTM D785
Tensile Strength, Ultimate 40.0 MPa
5800 psi
ASTM D638-61T
Elongation at Break 25 %
25 %
ASTM D638-61T
Izod Impact, Notched 1.17 J/cm
2.19 ft-lb/in
ASTM D256-56
0.270 J/cm

@Temperature -40.0 °C
0.506 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 151 °C
304 °F
Flow temperature, ASTM D569-59
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C
190 °F
ASTM D648-56
Electrical Properties Metric English Comments
Dielectric Constant 3.18

@Frequency 10000 Hz
3.18

@Frequency 10000 Hz
ASTM D150-54T
3.23

@Frequency 1000 Hz
3.23

@Frequency 1000 Hz
ASTM D150-54T
Dissipation Factor 0.0072

@Frequency 1000 Hz
0.0072

@Frequency 1000 Hz
ASTM D150-54T
0.0127

@Frequency 10000 Hz
0.0127

@Frequency 10000 Hz
ASTM D150-54T