Thermal Properties Metric English Comments
Melting Point 160 - 266 °C
320 - 510 °F
Average value: 233 °C Grade Count:15
Overview of materials for Modified ETFE, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Modified ETFE, Unreinforced". Each property range of values reported is minimum and maximum values of ap..