Thermal Properties Metric English Comments
Specific Heat Capacity 1.50 - 2.10 J/g-°C
0.359 - 0.502 BTU/lb-°F
Average value: 1.70 J/g-°C Grade Count:5
Overview of materials for Nylon 66, Glass/Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of..
Specific Heat Capacity 2.00 - 2.10 J/g-°C
0.478 - 0.502 BTU/lb-°F
Average value: 2.01 J/g-°C Grade Count:9
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max..