Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -116 °C
-177 °F
silicone property; ASTM E 1356
Arlon Thermabond® 99000W008 Silicone Rubber/Fiberglass Laminate
Low outgassing, thermally conductive, electrically insulating, Thermabond®. Bonds with primer. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass.
Glass Transition Temp, Tg -116 °C
-177 °F
silicone property; ASTM E 1356
Arlon Thermabond® 99000W015 Silicone Rubber/Fiberglass Laminate
Low outgassing, thermally conductive, electrically insulating, Thermabond®. Bonds with primer. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass.
Glass Transition Temp, Tg -116 °C
-177 °F
ASTM E1356
Arlon Thermabond® 99720W015 0.015" Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Design/Construction:Liner: 0.001" FEP FilmSide 1: Uncured Silicone RubberCarrier: 0.003" PTFE coated FiberglassRecommended Primer: Dow Corning S2260This data represents typical values for the pr..
Glass Transition Temp, Tg -116 °C
-177 °F
Silicone Property; ASTM E 1356
Arlon Thermabond® 99730N004 0.004" (0.102 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: Electrically Conductive - Thermabond®. Bonds with primer.Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Primers: Dow Coring..
Glass Transition Temp, Tg -116 °C
-177 °F
Silicone Property; ASTM D1356
Arlon Thermabond® 99730N015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: Electrically Conductive - Thermabond®. Bonds with primer.Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Primers: Dow Coring..
Glass Transition Temp, Tg -116 °C
-177 °F
silicone property; ASTM E 1356
Arlon Thermabond® 99950N008 Silicone Rubber/Fiberglass Laminate
Electrically conductive, Thermabond®. primerless. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass.
Glass Transition Temp, Tg -116 °C
-177 °F
silicone property; ASTM E 1356
Arlon Thermabond® 99950N015 Silicone Rubber/Fiberglass Laminate
Electrically conductive, Thermabond®. primerless. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass.
Glass Transition Temp, Tg -116 °C
-177 °F
Silicone Property; ASTM D1356
Arlon Thermabond® T20 (99710W008) 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: 8 mil thick Thermabond® T20 electrically insulating electronic adhesive.Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Prim..
Glass Transition Temp, Tg -116 °C
-177 °F
Silicone Property; ASTM D1356
Arlon Thermabond® T20 (99710W015) 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: 15 mil thick Thermabond® T20 electrically insulating electronic adhesive.Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Pri..
Glass Transition Temp, Tg -116 °C
-177 °F
Arlon SQA-TMS-055
Arlon R3792-920-10R##-P0 Silicone Rubber
This self-fusible silicone tape is specially formulated to yield improved flexibility, elongation and elastic recovery at low operating temperature (-70°C to -100°C) where standard fusible silicon..