Arlon Thermabond® 99000W008 Silicone Rubber/Fiberglass Laminate

Category Polymer , Adhesive , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name Thermabond®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon Thermabond® 99000W008 Silicone Rubber/Fiberglass Laminate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Low outgassing, thermally conductive, electrically insulating, Thermabond®. Bonds with primer. Liner: 1 mil FEP; Product: uncured silicone rubber; Carrier: 3 mil PTFE coated fiberglass.
Physical Properties Metric English Comments
Specific Gravity 1.70 g/cc
1.70 g/cc
silicone property; Arlon SQA-TMS-024
Thickness 203 microns
8.00 mil
overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
silicone property; ASTM D2240
Tensile Strength, Ultimate 2.07 MPa
300 psi
silicone property; ASTM D412
Elongation at Break 28 %
28 %
silicone property; ASTM D412
Modulus of Elasticity 0.0328 GPa
4.75 ksi
silicone property; Arlon SQA-TMS-008
Poissons Ratio 0.50
0.50
silicone property
Shear Modulus 0.448 GPa
65.0 ksi
silicone property; ASTM D1002
Shear Strength 1.28 MPa
185 psi
silicone property; ASTM D1002
Thermal Properties Metric English Comments
CTE, linear 110 µm/m-°C

@Temperature 20.0 °C
61.1 µin/in-°F

@Temperature 68.0 °F
silicone property; ASTM E 831
Specific Heat Capacity 0.700 J/g-°C
0.167 BTU/lb-°F
silicone property; ASTM E 1461-1
Thermal Conductivity 1.50 W/m-K
10.4 BTU-in/hr-ft²-°F
silicone property; ASTM E 1530
Maximum Service Temperature, Air 204 °C
400 °F
Minimum Service Temperature, Air -73.3 °C
-100 °F
Glass Transition Temp, Tg -116 °C
-177 °F
silicone property; ASTM E 1356
Electrical Properties Metric English Comments
Dielectric Constant 3.8

@Frequency 1.00e+6 Hz
3.8

@Frequency 1.00e+6 Hz
silicone property; IPC TM 650-2.5.5.3
Dielectric Strength 37.4 kV/mm
950 kV/in
ASTM D149
Dissipation Factor 0.0028

@Frequency 1.00e+6 Hz
0.0028

@Frequency 1.00e+6 Hz
silicone property; IPC TM 650-2.5.5.3
Processing Properties Metric English Comments
Cure Time 15.0 min

@Pressure 0.345 MPa,
Temperature 121 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 250 °F
Shelf Life 6.00 Month

@Temperature 7.22 °C
6.00 Month

@Temperature 45.0 °F
Descriptive Properties Value Comments
Color White
Users viewing this material also viewed the following: