Glass Transition Temp, Tg -25.0 °C
-13.0 °F
Second Run; DSC (-80°C to +100°C)
RedEye On Demand PolyJet™ Resin, Black, Rapid Prototyping Material
Tango PolyJet Resin (TangoGray™ FC950 & TangoBlack™ FC970) is a photopolymer resin designed for precise jetting in super fine layers by PolyJet™ Technology. Parts from the Tango PolyJet Resins si..
Glass Transition Temp, Tg -25.0 °C
-13.0 °F
Midpoint; ASTM E 1269
Huntsman IROGRAN® PS 443-201 TPU-Polyester
Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers
Glass Transition Temp, Tg -25.0 °C
-13.0 °F
Mallard Creek Polymers ROVENE® 4306 SBR Latex
ROVENE® 4306 is a carboxylated styrene-butadiene emulsion that has a soft, resilient hand with outstanding strength properties. This self-crosslinking binder imparts excellent water and solvent r..
Glass Transition Temp, Tg -25.0 °C
-13.0 °F
Mallard Creek Polymers ROVENE® 5550 SBR Latex
ROVENE® 5550 is a carboxylated styrene-butadiene emulsion that has a soft, resilient hand with outstanding strength properties. This Self-crosslinking binder imparts excellent water and solvent r..
Glass Transition Temp, Tg -25.0 °C
-13.0 °F
ASTM D1329
Seals Eastern 5353 Nitrile Rubber
General purpose NitrileInformation provided by Seals Eastern, Inc.
Glass Transition Temp, Tg -25.0 °C
-13.0 °F
ASTM D1329
Seals Eastern 7202 Nitrile Rubber
Nitrile for oil & gas serviceInformation provided by Seals Eastern, Inc.
Glass Transition Temp, Tg -25.0 °C
-13.0 °F
ASTM E1356
SK Chemicals SKYTHANE® U0417E Adhesive (Dry Lamination)
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
Glass Transition Temp, Tg -25.0 °C
-13.0 °F
ASTM D4065
SK Chemicals SKYTHANE® UB410 Powder Coating
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. UB series are used for adhesives and coating applications such as binder for magnetic ta..
Glass Transition Temp, Tg -25.0 °C
-13.0 °F
Styron XZ 92076.00 Carboxylated SB
Performance Features: Soft, good cellulosic binderApplications: Wipes and TissueEuropeInformation provided by Styron
Glass Transition Temp, Tg -25.0 °C
-13.0 °F
ASTM D1329
Seals Eastern 7157 Nitrile Rubber
Nitrile for oil & gas serviceInformation provided by Seals Eastern, Inc.
Glass Transition Temp, Tg -25.0 °C
-13.0 °F
HR 10 K/min, half height
Styron Sprintan® SLR 4601 Solution Styrene Butadiene Rubber (S-SBR)
Composition: SPRINTAN® SLR-4601 – Schkopau is manufactured by anionic solution polymerization using an organo-lithium initiator. The product has a medium styrene/high vinyl micro structure a..
Glass Transition Temp, Tg -25.0 °C
-13.0 °F
HR 10 K/min, half height
Styron Sprintan® SLR 4602 Solution Styrene Butadiene Rubber (S-SBR)
Composition: SPRINTAN® SLR-4602 – Schkopau is manufactured by anionic solution polymerization using an organo-lithium initiator. The product has a medium styrene/high vinyl micro structure a..
Glass Transition Temp, Tg -25.0 °C
-13.0 °F
ASTM D4065
SK Chemicals SKYTHANE® 410 Hotmelt Grade UB Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Glass Transition Temp, Tg -25.0 °C
-13.0 °F
Wanhua Chemical Wanthane® WHT-8264 Polyether-Based TPU
Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd.
Glass Transition Temp, Tg -25.0 °C
-13.0 °F
DSC
Lubrizol ESTANE® 58226 Ester Based Thermoplastic Polyurethane
Features: Excellent physical properties, good chemical resistance and enhanced hydrolysis resistance. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and..
Glass Transition Temp, Tg -25.0 °C
-13.0 °F
Lubrizol Estane® 2103-90A Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Low compression setAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 20..
Glass Transition Temp, Tg -25.0 - -18.0 °C
-13.0 - -0.400 °F
Eliokem Sunigum® P7395 Acrylate Terpolymer
Acrylate terpolymer partitioned with calcium carbonate. White powder; 1.00 mm particle size; medium viscosity.Intrinsically resistant to degradation by heat or UV radiation and to many chemicals in..
Glass Transition Temp, Tg -25.0 °C
-13.0 °F
HR 10 K/min; half height; DSC
Dow SE SLR-4601 Solution polymerized Styrene Butadiene Rubber (S-SBR)
SE SLR-4601 is manufactured by anionic solution polymerization using lithium initiator. It is a product with medium styrene and high vinyl content. The product is partially Sn-coupled and chemical..
Glass Transition Temp, Tg -25.0 °C
-13.0 °F
ASTM D1329
Seals Eastern 7168 Nitrile Rubber
Nitrile for oil & gas serviceInformation provided by Seals Eastern, Inc.