Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -30.0 °C | -22.0 °F | DSC, 10°C/min; DIN 51.007 |
Lubrizol Advanced Materials Pearlthane® ECO D20N55D Thermoplastic Polyurethane
(discontinued **) PEARLTHANE® ECO D20N55D is a 55 Shore D, High Performance natural TPU based on Renewable Sources with ca. 35% renewable content according to ASTM D6866 for Extrusion and Injection Molding applicati.. |
|||
Glass Transition Temp, Tg | -30.0 °C | -22.0 °F | DSC, 10ºC/min; DIN 51.007 |
Lubrizol Advanced Materials PEARLTHANE® 12K85A Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 12K85A is a standard polyester-based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties. It can be e.. |
|||
Glass Transition Temp, Tg | -30.0 °C | -22.0 °F | DMTA |
Solvay Specialty Polymers Solef® 31008 PVDF Copolymer
(discontinued **) Key features of this grade: High Flexibility/ High Elongation/Cold Impact Resistance, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General .. |
|||
Glass Transition Temp, Tg | -30.0 °C | -22.0 °F | DSC, 10ºC/min; DIN 51.007 |
Lubrizol Advanced Materials PEARLTHANE® 12F75UV Thermoplastic Polyurethane Elastomer PEARLTHANE® D12F75UV is a UV resistant standard polyester based TPU supplied in form of translucent, colorless or slightly yellowish pellets, featuring a low melting point and very low gel conten.. |
|||
Glass Transition Temp, Tg | -30.0 °C | -22.0 °F | |
Styron DL 219NA Carboxylated SB Performance Features: Soft polymer for excellent adhesion, tack coatApplications: Dust Control, Playground, Running Track, Soil Stabilization and Sound DampeningNorth AmericaInformation provided by .. |
|||
Glass Transition Temp, Tg | -30.0 °C | -22.0 °F | |
Styron DL 220NA Carboxylated SB Performance Features: Soft polymer for excellent adhesion, excellent water resistance, tack coat, excellent acoustic propertiesApplications: Dust Control, Playground, Running Track, Soil Stabilizati.. |
|||
Glass Transition Temp, Tg | -30.0 °C | -22.0 °F | |
Styron DL 220NA SAN Resin Performance Features: Flex and fold durability, high internal bond strengthApplications: General purpose and PSANorth AmericaInformation provided by Styron |
|||
Glass Transition Temp, Tg | -30.0 °C | -22.0 °F | |
Styron DL 2219LA Carboxylated SB Performance Features: General purpose, high adhesion to paper and olefin substrates, medium stiffnessApplications: General Purpose AdhesiveLatin America/South AmericaInformation provided by Styron |
|||
Glass Transition Temp, Tg | -30.0 °C | -22.0 °F | |
Styron DL 2219LA Carboxylated SB Performance Features: Multi purpose, balance of hot and wet tensile, high temperature tear resistance, high film elongationApplications: Fiber Binding and NonwovensEuropeInformation provided by Styr.. |
|||
Glass Transition Temp, Tg | -30.0 °C | -22.0 °F | |
Styron DL 220NA Carboxylated SB Performance Features: Good binding, flexible mineral sheetApplications: Flooring Felt and Leather BindingNorth AmericaInformation provided by Styron |
|||
Glass Transition Temp, Tg | -30.0 °C | -22.0 °F | DSC |
Lubrizol Estane® ZHF 95AT3 Thermoplastic Polyurethane, Flame Retardant Type: Estane® ZHF 95AT3 TPU is a zero halogen flame retardant polyether based thermoplastic polyurethane compound.Features: Outstanding flame retardant properties, especially suited for tray cables.. |
|||
Glass Transition Temp, Tg | -30.0 °C | -22.0 °F | |
Lubrizol Pellethane® 2363-90A Thermoplastic Polyurethane Elastomer Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Glass Transition Temp, Tg | -30.0 °C | -22.0 °F | |
Wanhua Chemical Wanthane® WHT-8254 Polyether-Based TPU Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Glass Transition Temp, Tg | -30.0 °C | -22.0 °F | DSC |
Lubrizol Estane® CP80AS2 Thermoplastic Polyurethane Type: Estane® CP80AS2 is a soft, polyester based thermoplastic polyurethane resin.Features: Outstanding compatibility with flexible PVC allowing easy dispersion without pre-compounding.Uses: Tube/H.. |
|||
Glass Transition Temp, Tg | -30.0 °C | -22.0 °F | 10°C/min |
Covestro Texin® 185 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionCoatingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialSc.. |
|||
Glass Transition Temp, Tg | -30.0 °C | -22.0 °F | DMTA |
Solvay Specialty Polymers Solef® 1008 PVDF Homopolymer
(discontinued **) Key features of this grade: Low Viscosity, All Purpose, Injection, Virgin. Recommended processing is injection. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF .. |
|||
Glass Transition Temp, Tg | -30.0 °C | -22.0 °F | DMTA |
Solvay Specialty Polymers Solef® 1010 PVDF Homopolymer
(discontinued **) Key features of this grade: Med Viscosity, All Purpose, Extrusion, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF .. |
|||
Glass Transition Temp, Tg | -30.0 °C | -22.0 °F | DMTA |
Solvay Specialty Polymers Solef® 1012 PVDF Homopolymer
(discontinued **) Key features of this grade: High Viscosity, Virgin. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-c.. |
|||
Glass Transition Temp, Tg | -30.0 °C | -22.0 °F | DSC |
Lubrizol ESTANE® 58213 Ester Based Thermoplastic Polyurethane Features: Excellent blend partner for PVC and general adhesive and good physical properties.Uses: Flat die/cast film extrusion and hose jacketing, Calendaring/melt coating.Available in Americas, Eur.. |
|||
Glass Transition Temp, Tg | -30.0 °C | -22.0 °F | DSC |
Lubrizol ESTANE® 58133 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUse: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and Asia Information provided by Lubrizol. |