Thermal Properties Metric English Comments
Glass Transition Temp, Tg -34.0 °C
-29.2 °F
ASTM D3417
REXtac Rextac® RT 4460 Amorphous Polyalphaolefin (APAO)
Wire and Cable Grade.Description: Ethylene copolymer and FDA compliantFeatures: Balance high temperature resistance and low temperature flexibilityApplications: Wire and Cable fillings and flooding ..
Glass Transition Temp, Tg -34.0 °C
-29.2 °F
Dow Pellethane® 2103-90AEN Polyurethane Elastomer, Ether Based  (discontinued **)
PELLETHANE® 2103-90AEN is a polytetramethylene glycol ether based polyurethane elastomer featuring superior resilience, low temperature properties, excellent hydrolytic stability, and resistance to..
Glass Transition Temp, Tg -34.0 °C
-29.2 °F
Midpoint; ASTM E 1269
Huntsman IROGRAN® PS 456-202 TPU-Polyester
Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers
Glass Transition Temp, Tg -34.0 °C
-29.2 °F
Lubrizol Estane® 2103-90AE Thermoplastic Polyurethane Elastomer
Formerly PellethaneAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
Glass Transition Temp, Tg -34.0 °C
-29.2 °F
10°C/min
Arkema Group Kynar® FLEX 2750 PVDF  (discontinued **)
Designation ISO 12086-VDF/HFP-K, EG1NS, M. ?E7.B.F.A.C,, ? (4-10)Kynar FLEX PVDF are fluorinated thermoplastic copolymers.Outstanding characteristics of Kynar FLEX: chemical resistance, imperviousne..
Glass Transition Temp, Tg -34.0 °C
-29.2 °F
DSC
Lubrizol Estane® 2103-90AENH Film Grade Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: NSF Standard 61 Certified, FDA ComplianceAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by Lubrizol.Lubrizol acquired the Pellethane prod..
Glass Transition Temp, Tg -34.0 °C
-29.2 °F
Compound
KKPC KOSYN SOL 5520 Solution Styrene Butadiene Rubber (S-SBR)
Solution Styrene Butadiene Rubber (S-SBR)Characteristics: This product is made by solution polymerization under which styrene and butadiene react in organic solvent using alkyl-lithium catalyst. It ..