Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 131 °C | 268 °F | Wet |
Hexcel® HexPly® F593 Epoxy Resin HexPly® F593 is a modified 350°F (177°C) curing epoxy system with very low flow for carbon fabric and tape applications that provides excellent laminate and honeycomb sandwich properties. As a lo.. |
|||
Glass Transition Temp, Tg | >= 131 °C | >= 268 °F | Post-Cure Dynamic Scan 20200°C; Ramp -40200°C @ 20°C/Min |
Epoxy Technology EPO-TEK® OG198-54 UV Cure Optical Epoxy Material Description: Single component, low viscosity, high Tg, UV curable epoxy. Active alignment of optics, securing fibers into V-grooves and fiber pigtails are a few of its common applications... |