Thermal Properties Metric English Comments
Glass Transition Temp, Tg 131 °C
268 °F
Wet
Hexcel® HexPly® F593 Epoxy Resin
HexPly® F593 is a modified 350°F (177°C) curing epoxy system with very low flow for carbon fabric and tape applications that provides excellent laminate and honeycomb sandwich properties. As a lo..
Glass Transition Temp, Tg >= 131 °C
>= 268 °F
Post-Cure Dynamic Scan 20200°C; Ramp -40200°C @ 20°C/Min
Epoxy Technology EPO-TEK® OG198-54 UV Cure Optical Epoxy
Material Description: Single component, low viscosity, high Tg, UV curable epoxy. Active alignment of optics, securing fibers into V-grooves and fiber pigtails are a few of its common applications...