Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3418 |
NatureWorks® Ingeo™ 2003D General Purpose Transparent Extrusion Grade Biopolymer NatureWorks® PLA polymer 2003D is a thermoplastic resin derived from annually renewable resources. PLA polymer 2003D processes easily on conventional extrusion equipment. Specifically designed fo.. |
|||
Glass Transition Temp, Tg | 55.0 - 65.0 °C | 131 - 149 °F | ASTM D3417 |
NatureWorks® Ingeo™ 3251D Injection Grade PLA IngeoTM Biopolymer 3251D is designed for injection molding applications. This polymer grade has a higher melt flow capability than other IngeoTM resins currently in the market place. The higher flow.. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3417 |
NatureWorks® Ingeo™ 6060D Fiber Grade PLA NatureWorks PLA polymer 6060D is an amorphous thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6060D is designed for extrusion into mech.. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3417 |
NatureWorks® Ingeo™ 6201D Fiber Grade PLA NatureWorks® PLA polymer 6201D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6201D is designed for extrusion into mechanically .. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3417 |
NatureWorks® Ingeo™ 6251D Fiber Grade PLA NatureWorks® PLA polymer 6251D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6251D is designed for spunbond products using conv.. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3417 |
NatureWorks® Ingeo™ 6302D Fiber Grade PLA NatureWorks PLA polymer 6302D is an amorphous thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6302D is designed for extrusion into mech.. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3417 |
NatureWorks® Ingeo™ 7032D Stretch Blow Molding/Bottle Grade PLA NatureWorks® PLA polymer 7032D is a bottles grade resin designed for injection stretch blow molded applications where heat setting is needed. PLA polymer 7032D can be run on conventional ISBM equip.. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3418 |
NatureWorks® Ingeo™ 8052D Foam Grade Biopolymer Ingeo 8052D can be converted into an expanded foam sheet with use temperatures up to 77°F (25°C). This foam is lightweight, strong and suitable for packaging fresh meat and vegetables. In order to.. |
|||
Glass Transition Temp, Tg | 55.0 °C | 131 °F | DSC, both heating and cooling speeds of 20°C/min |
Noltex Soarnol® A4412 Ethylene Vinyl Alcohol Copolymer Ethylene content 44 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a.. |
|||
Glass Transition Temp, Tg | 55.0 °C | 131 °F | DSC, both heating and cooling speeds of 20°C/min |
Noltex Soarnol® AT4403 Ethylene Vinyl Alcohol Copolymer High ethylene content, low melting point. Suitable for use in multilayer structures where ease of thermoforming is required. Ethylene content 44 mol%.The gas barrier property of Soarnol is about fo.. |
|||
Glass Transition Temp, Tg | 55.0 °C | 131 °F | 10°C/min; ISO 11357-1/-2 |
DuPont Performance Polymers Crastin® S600F20 NC010 PBT
(Unverified Data**) Crastin® S600F20 NC010 is an unreinforced, lubricated, medium viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3417 |
NatureWorks® Ingeo™ 6350D Fiber Grade PLA NatureWorks PLA polymer 6350D is an amorphous thermoplastic spunbond-grade resin derived primarily from annually renewable resources. Available in pellet form, 6350D is designed for extrusion into s.. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3417 |
NatureWorks® Ingeo™ 6752D Spunbond Grade Biopolymer Sheath polymer for spunbound uses. NatureWorks® PLA polymer 6752D, a NatureWorks LLC product, is a thermoplastic fiber-grade resin de-rived from annually renewable resources. Available in pellet f.. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3418 |
NatureWorks® Ingeo™ 7001D ISBM Bottle Grade Biopolymer Ingeo biopolymer 7001D is a thermoplastic resin derived from annually renewable resources and is specifically designed for use in injection stretch blow molded (ISBM) bottle applications. Ingeo biop.. |
|||
Glass Transition Temp, Tg | 55.0 °C | 131 °F | Dynamic Viscoelasticity |
EVALCA EVAL® LC-E105A Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 44 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, melt phase forming, solid phase pressure forming, tubes, coex coating. EVOH is used in packaging applications because of its out.. |
|||
Glass Transition Temp, Tg | 55.0 °C | 131 °F | Dynamic Viscoelasticity |
EVALCA EVAL® LC-E151B Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 44 mol % Ethylene.Data provided by EVALCA. Applications: Melt phase forming, solid phase pressure forming, blow molding, tubes EVOH is used in packaging applications because of its outstanding gas.. |
|||
Glass Transition Temp, Tg | 55.0 °C | 131 °F | |
Styron DL 295 Carboxylated SB Performance Features: General purpose wood adhesiveApplications: General Purpose Adhesive and Wood Adhesive (EPI)EuropeInformation provided by Styron |
|||
Glass Transition Temp, Tg | 55.0 °C | 131 °F | 10°C/min; ISO 11357-1/-2 |
DuPont Performance Polymers Crastin® FGS600F10 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Polybutylene Terephthalate Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Glass Transition Temp, Tg | 55.0 °C | 131 °F | 10°C/min; ISO 11357-1/-2 |
DuPont Performance Polymers Crastin® FGS600F40 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Low Viscosity Polybutylene Terephthalate Developed for Food Contact Applications Crastin FGS600F40 NC010 is an unreinforced low viscosity polybutylene terephthalate resin for injection .. |
|||
Glass Transition Temp, Tg | >= 55.0 °C | >= 131 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min |
Epoxy Technology EPO-TEK® 730 General Purpose Epoxy Product Description: EPO-TEK® 730 is a two component, thixotropic, room temperature-curing epoxy adhesive. Advantages & Application Notes: Excellent all purpose adhesive. Many uses in job shop and .. |
|||
Glass Transition Temp, Tg | >= 55.0 °C | >= 131 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min |
Epoxy Technology EPO-TEK® 731 Epoxy Adhesive Material Description: A two component, thixotropic, room temperature-curing epoxy adhesive. It is an electrically and thermally insulating epoxy designed for general applications in semiconductor p.. |
|||
Glass Transition Temp, Tg | >= 55.0 °C | >= 131 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min |
Epoxy Technology EPO-TEK® OE121 Black Epoxy Adhesive Material Description: A two component, low temperature curing epoxy adhesive designed for semiconductor flip chip underfill. It is color coded black for visual ID during the underfilling process. .. |
|||
Glass Transition Temp, Tg | 55.0 °C | 131 °F | |
Armstrong A-7 Epoxy Adhesive Clear, flexible, 5-minute cure structural bonding plastic adhesive. Develops high performance, high impact durable bonds for operating temperatures from -65° to +250°. Supplied in 1:1 ratio dispe.. |
|||
Glass Transition Temp, Tg | 55.0 °C | 131 °F | TM R050-25 |
Resinlab® EP1115 Clear Unfilled Epoxy Adhesive Resinlab™ EP1115 Clear is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. This product gives good resistance to water, salt spray, inorganic acids and.. |
|||
Glass Transition Temp, Tg | 55.0 °C | 131 °F | |
Loctite® Durabond® E-60NC Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |