Polymer Property : Glass Transition Temp, Tg = 138 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg >= 138 °C
>= 280 °F
DMA
Metton LMR M1534 Liquid Molding Resin
Different product numbers represent different formulations for customer specific needs such as liquid freezing point. Metton LMR is a tough and durable engineering plastic material used to produce ..
Glass Transition Temp, Tg 138 °C
280 °F
ASTM D3418
Lubrizol Isoplast® 202LGF40 Engineering Thermoplastic Polyurethane Resin
Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
Glass Transition Temp, Tg 138 °C
280 °F
10°C/min; ISO 11357-1,-2,-3
Topas Advanced Polymers TOPAS® 6013F-04 Cyclic Olefin Copolymer (COC)
TOPAS® 6013F-04 is a high temperature, general purpose film extrusion grade. It is a high clarity amorphous resin with high stiffness, moisture barrier, chemical resistance, thermoformability and p..
Glass Transition Temp, Tg 138 °C
280 °F
10°C/min; ISO 11357-1,-2,-3
Topas Advanced Polymers TOPAS® 6013S-04 Cyclic Olefin Copolymer (COC)
TOPAS® 6013S-04 is a general purpose injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance,..
Glass Transition Temp, Tg 138 °C
280 °F
ISO 11357-1, -2, -3
Topas Advanced Polymers TOPAS® IT X1 Cyclic Olefin Copolymer (COC)
TOPAS® IT X1 is an injection molding grade with heat and impact resistance. It is a moderately clear resin with high moisture barrier, chemical and heat resistance, making it suitable for products ..
Glass Transition Temp, Tg 138 °C
280 °F
Zeon Chemicals Zeonex® 480 Cyclo-Olefin Polymer
Glass Transition Temp, Tg 138 °C
280 °F
Zeon Chemicals Zeonex® 480R Cyclo-Olefin Polymer
Glass Transition Temp, Tg 138 °C
280 °F
ASTM D702807
Zyvex Performance Materials Arovex™ 250 Carbon Nanotube Strengthened Prepreg
Arovex® 250 Prepreg is a 180°F (82°C) to 280°F (138°C) curing carbon nanotube strengthened epoxy prepreg suitable for numerous composites applications. Normal curing takes place at 250°F (121°..