Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | >= 138 °C | >= 280 °F | DMA |
Metton LMR M1534 Liquid Molding Resin Different product numbers represent different formulations for customer specific needs such as liquid freezing point. Metton LMR is a tough and durable engineering plastic material used to produce .. |
|||
Glass Transition Temp, Tg | 138 °C | 280 °F | ASTM D3418 |
Lubrizol Isoplast® 202LGF40 Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Glass Transition Temp, Tg | 138 °C | 280 °F | 10°C/min; ISO 11357-1,-2,-3 |
Topas Advanced Polymers TOPAS® 6013F-04 Cyclic Olefin Copolymer (COC) TOPAS® 6013F-04 is a high temperature, general purpose film extrusion grade. It is a high clarity amorphous resin with high stiffness, moisture barrier, chemical resistance, thermoformability and p.. |
|||
Glass Transition Temp, Tg | 138 °C | 280 °F | 10°C/min; ISO 11357-1,-2,-3 |
Topas Advanced Polymers TOPAS® 6013S-04 Cyclic Olefin Copolymer (COC) TOPAS® 6013S-04 is a general purpose injection molding grade with a 130°C heat distortion temperature. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance,.. |
|||
Glass Transition Temp, Tg | 138 °C | 280 °F | ISO 11357-1, -2, -3 |
Topas Advanced Polymers TOPAS® IT X1 Cyclic Olefin Copolymer (COC) TOPAS® IT X1 is an injection molding grade with heat and impact resistance. It is a moderately clear resin with high moisture barrier, chemical and heat resistance, making it suitable for products .. |
|||
Glass Transition Temp, Tg | 138 °C | 280 °F | |
Zeon Chemicals Zeonex® 480 Cyclo-Olefin Polymer |
|||
Glass Transition Temp, Tg | 138 °C | 280 °F | |
Zeon Chemicals Zeonex® 480R Cyclo-Olefin Polymer |
|||
Glass Transition Temp, Tg | 138 °C | 280 °F | ASTM D702807 |
Zyvex Performance Materials Arovex™ 250 Carbon Nanotube Strengthened Prepreg Arovex® 250 Prepreg is a 180°F (82°C) to 280°F (138°C) curing carbon nanotube strengthened epoxy prepreg suitable for numerous composites applications. Normal curing takes place at 250°F (121°.. |