Thermal Properties Metric English Comments
Glass Transition Temp, Tg 69.0 °C
156 °F
Dynamic Viscoelasticity
EVALCA EVAL® F100 Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
32 mol % Ethylene.Data provided by EVALCA. Applications: Melt phase forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produced as a pa..
Glass Transition Temp, Tg 69.0 °C
156 °F
Dynamic Viscoelasticity
EVALCA EVAL® LC-F101BZ Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
32 mol % Ethylene.Data provided by EVALCA. Applications: Blown film, cast film, melt phase forming, blow molding, profile coextrusion. EVOH is used in packaging applications because of its outstan..
Glass Transition Temp, Tg 69.0 °C
156 °F
Dynamic Viscoelasticity
EVALCA EVAL® EP-F104BW Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
32 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, blow molding, tubes, coex coating. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL..
Glass Transition Temp, Tg 69.0 °C
156 °F
Dynamic Viscoelasticity
EVALCA EVAL® EP-J102B Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
32 mol % Ethylene.Data provided by EVALCA. Designed to provide a wide thermoforming range together with high barrier properties. EVAL® EP-J102B is specifically designed for thermoforming applicat..
Glass Transition Temp, Tg 69.0 °C
156 °F
Mallard Creek Polymers ROVENE® 4106 SBR Latex
ROVENE® 4106 is a carboxylated styrene-butadiene emulsion that has a very stiff or "boardy" hand. This binder is recommended as a modifier for other SBR non-woven binders to increase strength and..
Glass Transition Temp, Tg 69.0 °C
156 °F
Mallard Creek Polymers Rovene® 4111 Styrene-Butadiene Emulsion
Rovene® 4111 was designed with a specific particle size that greatly improves the spacing between titanium dioxide particles resulting in increased opacity. Additionally, using Rovene® 4111 ma..
Glass Transition Temp, Tg 69.0 °C
156 °F
ASTM D1525
Eastman Embrace LV Copolyester for Extruded/Cast Film
Applications:Beverage packagingDairy packagingFood packagingJuice packagingPharmaceutical packagingSoft drink packagingKey Attributes:Customizable shrink curveEye-catching 360° graphic capabilityLo..
Glass Transition Temp, Tg 69.0 °C
156 °F
ASTM D1525
Eastman Embrace LV Copolyester for Shrink Film
Applications:Beverage packagingDairy packagingFood packagingJuice packagingPharmaceutical packagingSoft drink packagingKey Attributes:Customizable shrink curveEye-catching 360° graphic capabilityLo..
Glass Transition Temp, Tg 69.0 °C
156 °F
ETM 300-90
ExxonMobil ESCOREZ™ 5320 Petroleum Hydrocarbon Resin
The Escorez 5300 series resins are water white cycloaliphatic hydrocarbon resins. They are designed to tackify a variety of adhesive polymers including EVA, SIS and SEBS block copolymers, APP an d A..
Glass Transition Temp, Tg 69.0 °C
156 °F
ASTM E1545-00
DSM Somos® ProtoGen™ 18920 Liquid Photopolymer, UV Postcure
Product DescriptionDSM Somos® ProtoGen 18920 is a liquid photopolymer that produces accurate, ABS-like parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demo..
Glass Transition Temp, Tg 69.0 °C
156 °F
dynamic; DIN 53 736
Hippe PET Polyethylene Terephthalate
Linear, saturated polyesters are thermoplastics which are used where good dimensional accuracy, high creep resistance and good sliding and wear behavior are required. Partially crystallized PET pos..
Glass Transition Temp, Tg 69.0 °C
156 °F
Dynamic Viscoelasticity
EVALCA EVAL® LC-T101 Ethylene Vinyl Alcohol Copolymer Resin  (discontinued **)
32 mol % Ethylene.Data provided by EVALCA. Applications: Solid phase pressure forming. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now produc..