Hippe PET Polyethylene Terephthalate

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer Erhard Hippe KG
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hippe PET Polyethylene Terephthalate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Linear, saturated polyesters are thermoplastics which are used where good dimensional accuracy, high creep resistance and good sliding and wear behavior are required. Partially crystallized PET possesses high hardness, strength at high temperatures and resistance against stress cracking.Information provided by Hippe.
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
DIN 53 479
Moisture Absorption at Equilibrium 0.30 %
0.30 %
Absorption of humidity in standard operating environment; DIN 53 715
Water Absorption at Saturation 0.50 %
0.50 %
DIN 53 495
Mechanical Properties Metric English Comments
Ball Indentation Hardness 145 MPa

@Time 30.0 sec
21000 psi

@Time 0.00833 hour
DIN 53 456
Tensile Strength 80.0 MPa
11600 psi
DIN 53 455
Elongation at Break 70 %
70 %
DIN 53 455
Tensile Modulus 2.80 GPa
406 ksi
DIN 53 457
Charpy Impact, Notched NB
NB
DIN 53 453
Coefficient of Friction, Dynamic 0.25
0.25
Against steel, p=0.05 N/mm², v=0.6 m/s, hardened and ground
Abrasion 0.35
0.35
µm/km; Against steel, p=0.05 N/mm², v=0.6 m/s, hardened and ground
Thermal Properties Metric English Comments
CTE, linear 70.0 - 80.0 µm/m-°C
38.9 - 44.4 µin/in-°F
Specific Heat Capacity 1.10 J/g-°C
0.263 BTU/lb-°F
Thermal Conductivity 0.240 W/m-K
1.67 BTU-in/hr-ft²-°F
Melting Point 255 °C
491 °F
DIN 53 736
Maximum Service Temperature, Air 110 °C
230 °F
Continuous use
180 °C
356 °F
Short Periods
Deflection Temperature at 0.46 MPa (66 psi) 170 °C
338 °F
ISO-R 75 Method B
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
ISO-R 75 Method A
Glass Transition Temp, Tg 69.0 °C
156 °F
dynamic; DIN 53 736
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
DIN 53 482, VDE 0303, Part 3
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
DIN 53 482
Dielectric Constant 3.2

@Frequency 1.00e+6 Hz
3.2

@Frequency 1.00e+6 Hz
DIN 53 483, IEC-250
Dielectric Strength 30.0 kV/mm
762 kV/in
Breakdown; DIN 53 481, IEC-243, VDE 0303 Part 1
Dielectric Loss Index 0.021

@Frequency 1.00e+6 Hz
0.021

@Frequency 1.00e+6 Hz
DIN 53 483, IEC-250
Descriptive Properties Value Comments
Color natural/black
Creep Resistance Grade CTI 350
DIN 53 480, IEC-112, VDE 0303 Part 1
Resistance to hot water, suds not resistant