Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 186 °C | 367 °F | DAM (SSYS) |
Proto3000 ULTEM* 9085 Fused Deposition Modeling Polymer Description: ULTEM* 9085 is a flame retardant high performance thermoplastic for direct digital manufacturing and rapid prototyping. It is ideal for the transportation industry due to its high stren.. |
|||
Glass Transition Temp, Tg | 186 °C | 367 °F | |
Stratasys® Ultem 9085 for Rapid Prototyping ULTEM* 9085 is a fl ame retardant high performance thermoplastic for direct digital manufacturing and rapid prototyping. It is ideal for the transportation industry due to its high strength-to-weigh.. |
|||
Glass Transition Temp, Tg | 186 °C | 367 °F | |
Master Bond UV25 One component, moderate viscosity UV curable system Product Description: Master Bond UV25 is a multi-purpose, one part UV curing system for bonding, sealing, coating and encapsulation that features excellent optical clarity, good physical properties,.. |