Stratasys® Ultem 9085 for Rapid Prototyping

Category Polymer , Rapid Prototyping Polymer , Thermoplastic , Polyetherimide (PEI)
Manufacturer Stratasys
Trade Name ULTEM
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Stratasys® Ultem 9085 for Rapid Prototyping.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ULTEM* 9085 is a fl ame retardant high performance thermoplastic for direct digital manufacturing and rapid prototyping. It is ideal for the transportation industry due to its high strength-to-weight ratio and its VØ rating for FST (fl ame, smoke, and toxicity). This unique material’s preexisting certifi cations make it an excellent choice for the commercial transportation industry – especially aerospace, marine and ground vehicles. Combined with a Fortus 3D Production System, ULTEM 9085 allows design and manufacturing engineers to produce fully functional parts that are ideal for advanced functional prototypes or end use without the cost or lead time of traditional tooling.Information provided by Stratasys.
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
Mechanical Properties Metric English Comments
Tensile Strength, Yield 71.64 MPa
10390 psi
Elongation at Yield 5.9 %
5.9 %
Tensile Modulus 2.22 GPa
322 ksi
Flexural Yield Strength 115 MPa
16700 psi
Flexural Modulus 2.500 GPa
362.6 ksi
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
Izod Impact, Unnotched 6.14 J/cm
11.5 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 153 °C
307 °F
Glass Transition Temp, Tg 186 °C
367 °F
Oxygen Index 49 %
49 %
Descriptive Properties Value Comments
FAA Flammability <5
FAR 25.853, method A/B
OSU Peak Heat Release 36 kW/m2
FAR25.853, 5 min test
OSU Total Heat Release 16 kW-min/m2
FAR25.853, 2 min test
Vertical Burn passes at 2 seconds
Test at 60s