Polymer Property : Glass Transition Temp, Tg = 293 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 83.0 - 145 °C
181 - 293 °F
Average value: 105 °C Grade Count:3
Overview of materials for Thermoset Polyurethane, Liquid
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid". Each property range of values reported is minimum and maximum values of..