Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 83.0 - 145 °C | 181 - 293 °F | Average value: 105 °C Grade Count:3 |
Overview of materials for Thermoset Polyurethane, Liquid This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid". Each property range of values reported is minimum and maximum values of.. |
|||
Glass Transition Temp, Tg | 83.0 - 100 °C | 181 - 212 °F | Average value: 90.5 °C Grade Count:6 |
Overview of materials for Polystyrene, Molded, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Glass Transition Temp, Tg | 83.0 °C | 181 °F | Plain Cast Resin; ASTM D3418 |
TSE Industries EcoWIND® M110 General Purpose Filament Winding Polyurethane Resin TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |
|||
Glass Transition Temp, Tg | 83.0 °C | 181 °F | Plain Cast Resin; ASTM D3418 |
TSE Industries EcoWIND® M110 General Purpose Filament Winding Polyurethane Resin TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |
|||
Glass Transition Temp, Tg | 83.0 °C | 181 °F | |
Eastman Eastar DN001 PCTG Copolyester ISO data as provided by the manufacturer, Eastman Chemical |
|||
Glass Transition Temp, Tg | 83.0 °C | 181 °F | |
Eastman Eastar DN004 PCTG Copolyester ISO data as provided by the manufacturer, Eastman Chemical |
|||
Glass Transition Temp, Tg | 83.0 °C | 181 °F | |
Armstrong A-12 Epoxy Adhesive, at 3:2 Mix Ratio Our most popular general-purpose, high viscosity adhesive for industry. Combines low toxicity with excellent physical properties, and offers a non-critical mixing ratio of 1:1 by weight. This rati.. |
|||
Glass Transition Temp, Tg | 83.0 °C | 181 °F | Ultimate Tg, 20°C/min; TMA |
Tra-Con Tra-Bond 970-1N1 General Purpose Epoxy Adhesive TRA-BOND 970-1N1 is a general purpose epoxy that exhibits sag resistance and excellent bond strength to a wide variety of substrates. Information provided by Tra-Con Inc. |