Polymer Property : Glass Transition Temp, Tg = 3.00 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 3.00 °C
37.4 °F
Mallard Creek Polymers TYLAC® 4190 SBR Emulsion
TYLAC® 4190 is a surfactant stabilized styrene-butadiene copolymer latex. When used in properly designed hydraulic cement mixtures, the addition of TYLAC® 4190 produces grouts, mortars, and c..
Glass Transition Temp, Tg 3.00 °C
37.4 °F
Styron XZ 92091.01 Cross-Linking SB
Performance Features: Excellent alkali resistance, low blockingApplications: Fiber Binding, Glass Fiber Binding and Performance CoatingsEuropeInformation provided by Styron
Glass Transition Temp, Tg 3.00 °C
37.4 °F
Unitika elitel UE3230 Polyester, Flake
Adhesive agent, Resin modifierUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesives, paints, ink binde..
Glass Transition Temp, Tg 3.00 °C
37.4 °F
Unitika elitel UE3231 Polyester, Flake
Molecular weight higher than UE3230, Improved solubilityUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as ad..
Glass Transition Temp, Tg 3.00 °C
37.4 °F
Onset
3M Scotch-Weld™ DP125 Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP125 Translucent is a faster curing version of 3M Scotch-Weld Epoxy Adhesive 2216 Translucent B/A. The worklife and cure time has been reduced from hours and days ..
Glass Transition Temp, Tg 3.00 °C
37.4 °F
TR10
3M Dyneon™ Aflas® FA-100H PTFE Fluoroelastomer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 57%F in polymer with 19% Medium Thermal Carbon Black (N990), 4% Triallyl Isocyanurate (TAIC), 1% Percadox™ 14, 1% Sodium..
Glass Transition Temp, Tg 3.00 °C
37.4 °F
TR10
3M Dyneon™ Aflas® FA-100S PTFE Fluoroelastomer  (discontinued **)
Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 57%F in polymer with 19% Medium Thermal Carbon Black (N990), 4% Triallyl Isocyanurate (TAIC), 1% Percadox™ 14, 1% Sodium..