Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 3.00 °C | 37.4 °F | |
Mallard Creek Polymers TYLAC® 4190 SBR Emulsion TYLAC® 4190 is a surfactant stabilized styrene-butadiene copolymer latex. When used in properly designed hydraulic cement mixtures, the addition of TYLAC® 4190 produces grouts, mortars, and c.. |
|||
Glass Transition Temp, Tg | 3.00 °C | 37.4 °F | |
Styron XZ 92091.01 Cross-Linking SB Performance Features: Excellent alkali resistance, low blockingApplications: Fiber Binding, Glass Fiber Binding and Performance CoatingsEuropeInformation provided by Styron |
|||
Glass Transition Temp, Tg | 3.00 °C | 37.4 °F | |
Unitika elitel UE3230 Polyester, Flake Adhesive agent, Resin modifierUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesives, paints, ink binde.. |
|||
Glass Transition Temp, Tg | 3.00 °C | 37.4 °F | |
Unitika elitel UE3231 Polyester, Flake Molecular weight higher than UE3230, Improved solubilityUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as ad.. |
|||
Glass Transition Temp, Tg | 3.00 °C | 37.4 °F | Onset |
3M Scotch-Weld™ DP125 Translucent Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP125 Translucent is a faster curing version of 3M Scotch-Weld Epoxy Adhesive 2216 Translucent B/A. The worklife and cure time has been reduced from hours and days .. |
|||
Glass Transition Temp, Tg | 3.00 °C | 37.4 °F | TR10 |
3M Dyneon™ Aflas® FA-100H PTFE Fluoroelastomer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 57%F in polymer with 19% Medium Thermal Carbon Black (N990), 4% Triallyl Isocyanurate (TAIC), 1% Percadox™ 14, 1% Sodium.. |
|||
Glass Transition Temp, Tg | 3.00 °C | 37.4 °F | TR10 |
3M Dyneon™ Aflas® FA-100S PTFE Fluoroelastomer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 57%F in polymer with 19% Medium Thermal Carbon Black (N990), 4% Triallyl Isocyanurate (TAIC), 1% Percadox™ 14, 1% Sodium.. |