Glass Transition Temp, Tg 150 - 343 °C
302 - 649 °F
Average value: 171 °C Grade Count:11
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and ..