Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 150 °C | 302 °F | ASTM D3482 |
Ovation Polymers Nemcon™ H PK DP110/X5 Polyetheretherketone Thermally Conductive Polyetheretherketone, excellent chemical, high stiffness, modulus and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All sa.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | TMA; IPC-TM-650.2.4.24c |
Park Electrochemical Nelco® N4000-7 SI® FR-4 Epoxy Laminate and Prepreg The Nelco® N4000-7 low-CTE epoxy laminate and prepreg system is a cost-effective solution for use in a broad range of multilayer PCB designs requiring low Z-axis expansion, excellent thermal stabil.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | ASTM D3418 |
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining most of.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | ASTM D3418 |
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical prope.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | ASTM D3418 |
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | ASTM D3418 |
Solvay Specialty Polymers KetaSpire® KT-820 NL Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 NL is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form. KetaSpire PEEK is produced to the highest industry standard.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | ASTM D3418 |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and pro.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | Midpoint; ISO 11357 |
Victrex® PEEK 450CA30 30% Carbon Fiber Reinforced General purpose, 30% carbon fiber reinforced, pelletized grade for injection molding.Information provided by Victrex. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | Midpoint; ISO 11357 |
Victrex® PEEK 450G General Purpose Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, FDA food contac.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | Midpoint; ISO 11357 |
Victrex® PEEK 450GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, F.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | Midpoint; ISO 11357 |
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | |
Cookson Group Plaskon® 3400FP Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A fast curing, reduced-stress epoxy molding compound for the encapsulation of semiconductor devices including DIPs, PLCCs, SOICs .. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | wet |
Henkel Hysol EA 9658 Film Adhesive High temperature and high durability film adhesive designed for high toughness and high temperature performanceApplications: Composite Bonding Metal and Honeycomb Bonding |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | dry |
Henkel Hysol EA 9895 WPP Peel Ply Pre-impregnated, polyester peel ply product supplied in film form. Specially designed resin system capable of curing at 350°F / 177°C. Compatible with state-of-the-art composite prepreg resin .. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | |
Ineos ABS Lustran® SMA 245 SMA Copolymer Lustran® SMA 245 is a Styrene Maleic Anhydride copolymer manufactured at a target maleic anhydride level of 25%. The process used for making Lustran® SMA 245 yields a product with good clarity.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | DSC |
Solvay Specialty Polymers Ajedium™ KT-820 Polyetheretherketone (PEEK) KetaSpire® KT-820 PEEK film is thermoplastic film that is characterized by a distinct combination of properties, which include excellent wear resistance, best-in-class fatigue resistance, high pu.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | DSC |
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK), 40% Glass Fiber AvaSpire® AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical ch.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | DSC |
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK) KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | DSC |
Solvay Specialty Polymers KetaSpire® KT-820FP Polyetheretherketone (PEEK) KetaSpire® KT-820FP is the low-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color fine powder form suitable for compression molding. KetaSpire® PEEK is produced.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | DSC |
Solvay Specialty Polymers KetaSpire® KT-820P Polyetheretherketone (PEEK) KetaSpire® KT-820P is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire® PEEK is produced to the highest industry standards.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | DSC |
Solvay Specialty Polymers KetaSpire® KT-851 Polyetheretherketone (PEEK) KetaSpire® KT-851 resin is a depth-filtered grade of polyetheretherketone (PEEK) specially designed for use in extruded wire insulation coating. KT-851 offers the needed balance of properties and.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | DSC |
Solvay Specialty Polymers KetaSpire® KT-XXXX Polyetheretherketone (PEEK) KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | |
Vyncolit Neopreg Kinel® SK61 L5G Glass Fiber Reinforced Molding Compound Epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particular suited for over molding.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | |
Cosmic Plastics E486 lass Filled Epoxy Molding Compound, Electrical Grade Data provided by the manufacturer. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | ISO 11357-1/-2 |
Covestro Makrolon® 3206 Polycarbonate ISO 7391-PC,M,(,,)-05-9MVR (300 °C/1.2 kg) 4.0 cm3/10 minFood contact qualityHigh viscosityGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CExtrusionAvailable in transpar.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | Midpoint; ISO 11357 |
Victrex® PEEK 650G Polyetheretherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | Midpoint; ISO 11357 |
Victrex® PEEK 450G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA food contac.. |