Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 150 °C | 302 °F | ASTM D3482 |
Ovation Polymers Nemcon™ H PK DP110/X5 PEEK Thermally Conductive Polyetheretherketone, excellent chemical, high stiffness, modulus and HDT.Information provided by Ovation Polymers |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | ASTM D3418 |
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been formula.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | ASTM D3418 |
Solvay Specialty Polymers AvaSpire® AV-722 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-722 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-722. This formulation offers improved part economics relative to 30% carbon fiber reinforced PEEK while retaining most of.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | ASTM D3418 |
Solvay Specialty Polymers KetaSpire® KT-820 CF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 CF30 is the low-flow, 30% carbon-fiber reinforced grade of polyetheretherketone (PEEK). Carbon- fiber reinforcement of KetaSpire PEEK provides the maximum levels of mechanical prope.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | ASTM D3418 |
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | ASTM D3417 |
Solvay Specialty Polymers KetaSpire® KT-820P Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820P is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire PEEK is produced to the highest industry standards and is .. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | ASTM D3418 |
Solvay Specialty Polymers KetaSpire® KT-850 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-850 is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color pellet form. KetaSpire PEEK is produced to the highest industry standards and .. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | Midpoint; ISO 11357 |
Victrex® PEEK 450FC30 General Purpose Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and ext.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | Midpoint; ISO 11357 |
Victrex® PEEK 450GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, F.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | Midpoint; ISO 11357 |
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | Midpoint; ISO 11357 |
Victrex® PEEK 450P Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, coarse powder for extrusion compounding, standard flow, FDA food contact comp.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | Midpoint; ISO 11357 |
Victrex® PEEK 450PF Fine Powder Grade Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for compression molding, standard flow, FDA food contact complia.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | Midpoint; ISO 11357 |
Victrex® PEEK 650CA30 30% Carbon Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, FDA food contact compliant.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | Midpoint; ISO 11357 |
Victrex® PEEK 650P PolyEtherEtherKetone High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, coarse powder for extrusion compounding, low flow, FDA food contact compliant, color natural.Info.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 1800 Unsaturated Polyester UP SMC 1800 is for structural applications requiring extreme high mechanical properties and low weight. These compounds mould to parts focussing on mechanical strength for replacement of metals in ord.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | |
Ineos ABS Lustran® SMA 245 SMA Copolymer Lustran® SMA 245 is a Styrene Maleic Anhydride copolymer manufactured at a target maleic anhydride level of 25%. The process used for making Lustran® SMA 245 yields a product with good clarity.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | DSC |
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK), 40% Glass Fiber AvaSpire® AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical ch.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | DSC |
Solvay Specialty Polymers KetaSpire® KT-820 Polyetheretherketone (PEEK) KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | DSC |
Solvay Specialty Polymers KetaSpire® KT-820P Polyetheretherketone (PEEK) KetaSpire® KT-820P is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire® PEEK is produced to the highest industry standards.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | DSC |
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK) KetaSpire® KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insula.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | DSC |
Solvay Specialty Polymers KetaSpire® KT-XXXX Polyetheretherketone (PEEK) KetaSpire® KT-820 is a low flow grade of unreinforced polyetheretherketone (PEEK) supplied in a lubricated pellet form. KetaSpire® PEEK is produced to the highest industry standards and is cha.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | |
Vyncolit Neopreg Kinel® SK61 L5G Glass Fiber Reinforced Molding Compound Epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particular suited for over molding.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | ISO 11357-1/-2 |
Covestro Makrolon® 3206 Polycarbonate ISO 7391-PC,M,(,,)-05-9MVR (300 °C/1.2 kg) 4.0 cm3/10 minFood contact qualityHigh viscosityGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CExtrusionAvailable in transpar.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | ISO 11357-1/-2 |
Covestro Makrolon® WB1239 Polycarbonate ISO 7391-PC,B,(,,)-05-9Global gradeMVR (300 °C/1.2 kg) 2.5 cm3/10 minBlow moldingHigh viscosityBranchedFood contact qualityExtrusion blow moldingInjection stretch blow moldingAvailable in transpare.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | Midpoint; ISO 11357 |
Victrex® PEEK 381G Medium Viscosity Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, depth filtered granules for specialty extrusion processes, standard flow, FD.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | Midpoint; ISO 11357 |
Victrex® PEEK 450CA20 Polyetheretherketone, 20% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | Midpoint; ISO 11357 |
Victrex® PEEK 450G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA food contac.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | Midpoint; ISO 11357 |
Victrex® PEEK 450GL15 Polyetheretherketone, 15% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 15% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, F.. |
|||
Glass Transition Temp, Tg | 150 °C | 302 °F | Midpoint; ISO 11357 |
Victrex® PEEK 650GL30 30% Glass Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, color natural/beige.Typical.. |