Thermal Properties Metric English Comments
Glass Transition Temp, Tg 78.0 - 80.0 °C
172 - 176 °F
PEPL-10-W-19
Pearl Engineering PEPLPET B-109JS PET Sheet Grade
Used mainly for 5 to 20 liter mineral water containers
Glass Transition Temp, Tg 78.0 - 80.0 °C
172 - 176 °F
PEPL-10-W-19
Pearl Engineering PEPLPET B-113C PET Sheet Grade
Used mainly for box strapping.
Glass Transition Temp, Tg 78.0 °C
172 °F
Eastman Eastapak 9921W PET  (discontinued **)
Unreinforced. ISO data as provided by the manufacturer, Eastman Chemical.This product is discontinued; 2003.
Glass Transition Temp, Tg 78.0 °C
172 °F
10°C/min; ISO 11357-1,-2,-3
Topas Advanced Polymers TOPAS® 8007D-61 Cyclic Olefin Copolymer (COC)
TOPAS® 8007D-61 is an externally lubricated version of our 8007 series of injection molding resins, targeting injection blow molding (IBM) and injection stretch blow molding (ISBM) applications. Li..
Glass Transition Temp, Tg 78.0 °C
172 °F
10°C/min; ISO 11357-1,-2,-3
Topas Advanced Polymers TOPAS® 8007F-04 Cyclic Olefin Copolymer (COC)
TOPAS® 8007F-04 is a general purpose film extrusion grade. It is a high clarity amorphous resin with high stiffness, moisture barrier, chemical resistance, thermoformability and purity for food and..
Glass Transition Temp, Tg 78.0 °C
172 °F
10°C/min; ISO 11357-1,-2,-3
Topas Advanced Polymers TOPAS® 8007S-04 Cyclic Olefin Copolymer (COC)
TOPAS® 8007S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma..
Glass Transition Temp, Tg 78.0 °C
172 °F
10°C/min; ISO 11357-1,-2,-3
Topas Advanced Polymers TOPAS® 8007X10 Cyclic Olefin Copolymer (COC)
TOPAS® 8007X10 is a highly UV-transparent version of our 8007 series of injection molding resins. Like the rest of the 8007 grades, 8007X10 is a glass-clear amorphous polymer with outstanding moist..
Glass Transition Temp, Tg 78.0 °C
172 °F
DSC
Wolf Kunststoff ZEDEX® ZX-100K A1K Polymer Alloy
Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good weather resistance; Good machinability; FDA compliant LABS; PTFE and silicone-free; KTW approved; Stress resistantApplications: ..
Glass Transition Temp, Tg 78.0 °C
172 °F
Ultimate Tg
Tra-Con Tra-Duct 2705 Room Temperature Conductive Nickel Epoxy Adhesive
TRA-DUCT 2705 is an electrically conductive nickel filled epoxy adhesive recommended for electronic bonding, sealing, and EMI-RFI shielding applications. This two-part smooth paste formulation is fr..
Glass Transition Temp, Tg 78.0 °C
172 °F
10°C/min; ISO 11357-1,-2,-3
Topas Advanced Polymers TOPAS® 8007F-400 Cyclic Olefin Copolymer (COC)
TOPAS® 8007F-400 is a robust film extrusion grade designed for blending with polyethylene (PE). It is a moderate clarity amorphous resin with high stiffness, moisture barrier, chemical resistance, ..
Glass Transition Temp, Tg 78.0 °C
172 °F
Eastman Eastapak 9921 PET
ISO data as provided by the manufacturer, Eastman Chemical
Glass Transition Temp, Tg 78.0 °C
172 °F
1/MA/1/007
Dow LIGHTER™ C88 Polyethylene Terephthalate (PET) Resin
LIGHTER™ resins are polyethylene terephthalate produced from PTA and MEG. These polymers are specifically designed for the production of beverage, food and other liquid containers and for thermofo..
Glass Transition Temp, Tg 78.0 °C
172 °F
1/MA/1/007
Dow LIGHTER™ C93 Polyethylene Terephthalate (PET) Resin
LIGHTER™ resins are polyethylene terephthalate produced from PTA and MEG. These polymers are specifically designed for the production of beverage, food and other liquid containers and for thermofo..
Glass Transition Temp, Tg 78.0 °C
172 °F
1/MA/1/007
Dow LIGHTER™ C98 Polyethylene Terephthalate (PET) Resin
LIGHTER™ resins are polyethylene terephthalate produced from PTA and MEG. These polymers are specifically designed for the production of beverage, food and other liquid containers and for thermofo..
Glass Transition Temp, Tg 78.0 °C
172 °F
1/MA/1/007
Dow LIGHTER™ S93 Polyethylene Terephthalate (PET) Resin
LIGHTER™ S93 is a polyester polymer modified to improve infrared reheating of preforms. It provides very good mechanical properties and a wide processing range on all injection molding machines. ..
Glass Transition Temp, Tg 78.0 °C
172 °F
1/MA/1/007
Dow LIGHTER™ S98 Polyethylene Terephthalate (PET) Resin
LIGHTER™ S98 is a polyester polymer modified to improve infrared reheating of preforms. It provides very good mechanical properties and a wide processing range on all injection molding machines. ..