Tra-Con Tra-Duct 2705 Room Temperature Conductive Nickel Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy, Electrically Conductive , Filled/Reinforced Thermoset
Manufacturer Tra-Con, Inc.
Trade Name Tra-Duct
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Duct 2705 Room Temperature Conductive Nickel Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-DUCT 2705 is an electrically conductive nickel filled epoxy adhesive recommended for electronic bonding, sealing, and EMI-RFI shielding applications. This two-part smooth paste formulation is free of solvents, silver, copper or carbon additives, and is a low-cost replacement for many gold or silver based products. TRA-DUCT 2705 cures at room temperature and can be used as a "cold solder" for bonding and shielding heat sensitive components. TRA-DUCT 2705 is recommended for use where exposure to salt water causes silver based systems to corrode. It develops strong, durable bonds to substrates such as metal ceramic glass and plastic laminates.Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 3.20 g/cc
3.20 g/cc
Mixed
Viscosity 47500 cP

@Temperature 25.0 °C
47500 cP

@Temperature 77.0 °F
Resin (cp #52, 10 rpm)
Mechanical Properties Metric English Comments
Hardness, Shore D 88
88
1 hr @ 70°C
Adhesive Bond Strength 6.89 MPa
1000 psi
Lap shear, alum to alum, 1 hr @ 70°C
Thermal Properties Metric English Comments
Thermal Conductivity 1.40 W/m-K
9.72 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 130 °C
266 °F
Minimum Service Temperature, Air -54.0 °C
-65.2 °F
Glass Transition Temp, Tg 78.0 °C
172 °F
Ultimate Tg
Electrical Properties Metric English Comments
Volume Resistivity 0.0060 ohm-cm
0.0060 ohm-cm
cured 1 hr @ 70°C
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 70.0 °C
1.00 hour

@Temperature 158 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Descriptive Properties Value Comments
Color Clear
Hardener
Dark Gray
Resin/Mixed/Cured
Mix Ratio, parts by weight 100/5
Resin/Hardener
Thixotropic Index 3.9
1 rpm/10 rpm
Working Life minutes 40
10 grams