Thermal Properties Metric English Comments
Glass Transition Temp, Tg 82.0 - 121 °C
180 - 250 °F
Average value: 98.8 °C Grade Count:5
Overview of materials for PEN-PET
This property data is a summary of similar materials in the MatWeb database for the category "PEN-PET". Each property range of values reported is minimum and maximum values of appropriate MatWeb ent..
Glass Transition Temp, Tg 82.0 - 87.0 °C
180 - 189 °F
Average value: 84.0 °C Grade Count:8
Overview of materials for PCTG Copolyester
This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M..
Glass Transition Temp, Tg 82.0 °C
180 °F
Eastman Eastar DN102 PCTG Copolyester  (discontinued **)
ISO data as provided by the manufacturer, Eastman Chemical
Glass Transition Temp, Tg 82.0 °C
180 °F
Eastman Eastar DN101 PCTG Copolyester  (discontinued **)
ISO data as provided by the manufacturer, Eastman Chemical
Glass Transition Temp, Tg 82.0 °C
180 °F
DSC method
Honeywell Aegis™ HFX High Barrier Nylon  (discontinued **)
Description: Aegis® HFX is an oxygen scavenging polyamide composition formulated specifically for use in high performance packaging applications where high gas barrier is required. This product is ..
Glass Transition Temp, Tg 82.0 °C
180 °F
DSC method
Honeywell Aegis™ CSD High Barrier Nylon  (discontinued **)
Description: Aegis CSD provides delamination resistance during production and a significantly improved, high level of passive CO2 barrier compared with monolayer PET. Information provided by Honeyw..
Glass Transition Temp, Tg 82.0 °C
180 °F
DSC
Kolon NOPLA® KE531 PEN-PET Copolyester
NOPLA® is an advanced PEN-PET copolyester which can be used for bottle, sheet & injection molding applicationsUV protection & prolonged outdoor durability, enhanced gas barrier, outstanding impac..
Glass Transition Temp, Tg 82.0 °C
180 °F
TMA
Lord Adhesives Thermosetâ„¢ MD-140 Conductive Adhesive
LORD Thermosetâ„¢ MD-140 silver-filled conductive adhesive offers excellent thermal conductivity. It is designed for use in thermally demanding die attach applications such as microprocessor, po..
Glass Transition Temp, Tg 82.0 °C
180 °F
Ultimate Tg
Tra-Con Tra-Cast 3156 General Purpose Epoxy Casting System
TRA-CAST 3156 is an easy-to-use, low cost, versatile epoxy resin and hardener system developed for general purpose casting applications. It develops excellent adhesion to most metals, plastics, and ..
Glass Transition Temp, Tg 82.0 °C
180 °F
DSC
Eastman Cadence™ GS2 Copolyester for film calendering
Eastman Cadence™ copolyester, for calendered films, is a specialty plastic developed to meet the demand for an environmentally responsible material for the calendering industry. Available in diffe..
Glass Transition Temp, Tg 82.0 °C
180 °F
Epoxyset Epoxibond EB-309 Low Expansion Epoxy Adhesive
EB-309 is a highly filled, extremely low expansion, epoxy adhesive. This low out-gassing adhesive exhibits excellent wettability without preheating metal bonding surfaces and has a good dimensional ..
Glass Transition Temp, Tg 82.0 °C
180 °F
TM R050-25
Resinlab® EP1199 Black Unfilled Epoxy Adhesive
Resinlab™ EP1199 Black is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. This product gives good resistance to water, salt spray, inorganic acids and..
Glass Transition Temp, Tg 82.0 °C
180 °F
TM R050-25
Resinlab® EP1199 Clear Unfilled Epoxy Adhesive
Resinlab™ EP1199 Clear is a two part unfilled epoxy adhesive designed for bonding of metals, ceramics and most plastics. This product gives good resistance to water, salt spray, inorganic acids and..