Polymer Property : CTE, linear, Transverse to Flow = 10.0 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 18.0 - 66.0 µm/m-°C
10.0 - 36.7 µin/in-°F
Average value: 39.7 µm/m-°C Grade Count:5
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an..
CTE, linear, Transverse to Flow 18.0 µm/m-°C

@Temperature 20.0 °C
10.0 µin/in-°F

@Temperature 68.0 °F
Crosswise; ASTM D696
G-9 Fiberglass Melamine Laminate Sheet
This material is very hard, flame resistant, and has excellent electrical properties. G-9 has high arc and heat resistance and is recommended for humid environments. It is used for switch board pane..
CTE, linear, Transverse to Flow 18.0 µm/m-°C

@Temperature 20.0 °C
10.0 µin/in-°F

@Temperature 68.0 °F
Crosswise; ASTM D696
G-3 Fiberglass Phenolic Laminate Sheet
This material is made from woven glass cloth and high-temperature phenolic resin. It has excellent flexural, compressive and impact strengths. Physical strength, resiliency, ease and versatility of ..
CTE, linear, Transverse to Flow 18.0 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
10.0 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis
Industrial Laminates/Norplex NP841 Glass Fabric  (discontinued **)
Description: Woven glass fabric with phenolic resin. Contains Kocite® for controlled conductivity. Acts as static electricity drain to protect electrical and electronic equipment.Thickness Tested: ..
CTE, linear, Transverse to Flow 18.0 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
10.0 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis; IPC-TM 650-2.4.24
Industrial Laminates/Norplex NP504 Glass Fabric
Description: Woven glass fabric with high temperature phenolic resin. Good flexural, compressive and impact strengths at elevated temperatures. Capable of continuous operation at 175° C, see note..
CTE, linear, Transverse to Flow 18.0 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
10.0 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis; IPC-TM 650-2.4.24
Industrial Laminates/Norplex NP509 Glass Fabric
Description: Woven glass fabric, melamine resin laminate. Very hard, flame resistant, machining grade with excellent electrical properties in high humidity conditions. High physical strength and exc..
CTE, linear, Transverse to Flow 18.0 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
10.0 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis; IPC-TM 650-2.4.24
Industrial Laminates/Norplex NP664 Paper Base Laminate
Description: Low cost room temperature punching grade with mechanical and electrical properties similar to NP612. This version is made with pigment cover plies on the surface.Thickness Tested: 0.062..
CTE, linear, Transverse to Flow 18.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
10.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Noryl TN240 PPE+PS
PPE+PS blend. Unfilled. Transparent. Good flow. Scratch resistant. Injection molding. Suitable for housewares, personal care and small appliance applications.This data was supplied by SABIC-IP for t..
CTE, linear, Transverse to Flow 18.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
10.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Noryl TN240 PPE+PS (Asia Pacific)
PPE+PS. Transparent. High flow, scratch resistant. Injection molding. Housewares and small appliances applications.This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Transverse to Flow 18.0 µm/m-°C

@Temperature -30.0 - 100 °C
10.0 µin/in-°F

@Temperature -22.0 - 212 °F
ISO 11359-2
SABIC Innovative Plastics SABIC PPCOMPOUND 7985 PP
SABIC® PPcompound 7985 is a mineral filled, impact modified polypropylene TPO. This material combines scratch resistance and heat stability with interior automotive UV stability. The IMDS is 2097..
CTE, linear, Transverse to Flow 18.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
10.0 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Stat-kon DE008E PC (Europe-Africa-Middle East)
LNP* Stat-kon* DE008E is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding.This data was supplied by SA..
CTE, linear, Transverse to Flow 18.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
10.0 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics Noryl PKN4766 PPE+PS (Asia Pacific)
PPE+PS. Translucent. FDA compliant. High flow. Extrusion. Microwavable. Food packaging uses.This data was supplied by SABIC-IP for the Asia Pacific region.
CTE, linear, Transverse to Flow 18.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
10.0 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 11359-1/-2
BASF Ultramid® KR 4355 G10 BK 23215 50% Glass Filled PA6/6T (Dry)
Description: 50% glass-fiber reinforced product for injection molding; high toughness and rigidity; low water absorption, high melting point (285°C); mechanical properties remain constant up to 60°..
CTE, linear, Transverse to Flow 18.0 µm/m-°C

@Temperature 20.0 °C
10.0 µin/in-°F

@Temperature 68.0 °F
Crosswise; ASTM D696
G-5 Fiberglass Melamine Laminate Sheet
This material is very hard, flame resistant, and has excellent electrical properties. G-5 has high arc and heat resistance. It used for switch board panels, arc barriers, circuit breaker parts, and ..
CTE, linear, Transverse to Flow 18.0 - 27.0 µm/m-°C
10.0 - 15.0 µin/in-°F
Average value: 23.0 µm/m-°C Grade Count:4
Overview of materials for Vinyl Ester Sheet Molding Compound
This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value..
CTE, linear, Transverse to Flow 18.0 µm/m-°C

@Temperature 20.0 °C
10.0 µin/in-°F

@Temperature 68.0 °F
XY-direction; ASTM D696
Premix Premi-Glas® 1285VE 1285 VE Glass Reinforced Vinyl Ester SMC  (discontinued **)
Description: Premi-Glas® 1285 VE is a glass reinforced vinyl ester sheet molding compound designed for automotive under the hood applications. Key features and benefits: Designed for compression mo..