Polymer Property : CTE, linear, Transverse to Flow = 100 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 180 µm/m-°C

@Temperature -30.0 - 30.0 °C
100 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM E831
PolyOne Edgetek® TR2-30GF/000 NATURAL Copolyester
The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea..
CTE, linear, Transverse to Flow 180 µm/m-°C

@Temperature 20.0 °C
100 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
DSM Stanyl® TW363 (DAM) Nylon 46 Heat Stabilized, Impact Modified (North America)
Information provided by DSM Engineering Plastics.
CTE, linear, Transverse to Flow 180 µm/m-°C

@Temperature 20.0 °C
100 µin/in-°F

@Temperature 68.0 °F
ISO 11359-1/-2
DSM Stanyl® TW363 Nylon 46 (European Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
CTE, linear, Transverse to Flow 180 µm/m-°C
100 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® L 25 W 20 Y PA12-I
Product Description: Grilamid L 25 W 20 Y black 9992 is a semiflexible plasticized, medium viscosity, extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 20 Y black 9992 is impact modified, heat..
CTE, linear, Transverse to Flow 180 µm/m-°C
100 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® L 25 W 40 X PA12-I
Product Description: Grilamid L 25 W 40 X is a flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 40 X is impact modified and heat and UV stabilized. The m..
CTE, linear, Transverse to Flow 180 µm/m-°C
100 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® L 22A W 40 X PA12-I
Product Description: Grilamid L 22A W 40 X is a flexible plasticized and impact modified heat and light stabilized Polyamide 12 (PA12). The main features of Grilamid L 22A W 40 X are: Good impact st..
CTE, linear, Transverse to Flow 180 µm/m-°C
100 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® L 25 W 20 X PA12-I
Product Description: Grilamid L 25 W 20 X is a semi-flexible plasticized high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 20 X is impact modified and UV and heat stabilized. Th..
CTE, linear, Transverse to Flow 180 µm/m-°C
100 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® L 25 W 40 ESD PA12
Product Description: Grilamid L 25 W 40 ESD is a high viscosity, anti-static highly flexible extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 40 ESD is plasticized and heat stabilized The inh..
CTE, linear, Transverse to Flow 180 µm/m-°C
100 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® L 25 W 40 HL X PA12-I
Product Description: Grilamid L 25 W 40 HLX is a flexible Polyamide 12 grade with an excellent cold impact strength and heat stability. Grilamid L 25 W 40 HLX is specially suitable for flexible tube..
CTE, linear, Transverse to Flow 180 µm/m-°C
100 µin/in-°F
ISO 11359-1/-2
EMS-Grivory Grivory® L 25 W 40 PA12
Product Description: Grilamid L 25 W 40 is a flexible, plasticised, high viscosity extrusion grade of Polyamide 12 (PA12) Grilamid L 25 W 40 is UV and heat stabilized. The main features of Grilamid ..
CTE, linear, Transverse to Flow 180 µm/m-°C

@Temperature 55.0 - 160 °C
100 µin/in-°F

@Temperature 131 - 320 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612  (Unverified Data**)
Unreinforced Polyamide 612Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 180 µm/m-°C

@Temperature 55.0 - 160 °C
100 µin/in-°F

@Temperature 131 - 320 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® 158L NC010 Nylon 612  (Unverified Data**)
Unreinforced Polyamide 612Information provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 180 µm/m-°C

@Temperature 23.0 - 60.0 °C
100 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Staramide BG4ST43 PA6, Glass Fiber Filled, Impact Modified, Injection Molded
Staramide BG4ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
CTE, linear, Transverse to Flow 180 µm/m-°C

@Temperature 20.0 - 60.0 °C
100 µin/in-°F

@Temperature 68.0 - 140 °F
TMS2 Perkin Elmer
Arkema Group Orgalloy® LT 5050 Polyamide Alloy
Polyamide Alloy, Flexible gradeTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group
CTE, linear, Transverse to Flow 180 µm/m-°C

@Temperature 55.0 - 160 °C
100 µin/in-°F

@Temperature 131 - 320 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® FG151L NC010 Nylon 612  (Unverified Data**)
Unreinforced Polyamide 612 with Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
CTE, linear, Transverse to Flow 180 µm/m-°C

@Temperature 20.0 - 60.0 °C
100 µin/in-°F

@Temperature 68.0 - 140 °F
TMS2 Perkin Elmer
Arkema Group Orgalloy® LT 5050 ES Polyamide Alloy
Polyamide Alloy, Blow Molding of Technical PartsInformation provided by Arkema Group