Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | XY Direction |
Premix Premi-Glas® 2206-15 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2206-15 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
CTE, linear, Transverse to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | XY Direction |
Premix Premi-Glas® 2206-22 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2206-22 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
CTE, linear, Transverse to Flow | 15.0 µm/m-°C | 8.33 µin/in-°F | XY Direction |
Premix Premi-Glas® 2206-25 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2206-25 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
CTE, linear, Transverse to Flow | 15.0 µm/m-°C @Temperature 20.0 °C |
8.33 µin/in-°F @Temperature 68.0 °F |
Crosswise; ASTM D696 |
G-11 Fiberglass Epoxy Laminate Sheet This glass-epoxy laminate is specified for its extremely high strength and high dimensional stability over temperature. G-11 is used for terminal boards, high humidity applications, electrical and e.. |
|||
CTE, linear, Transverse to Flow | 15.0 µm/m-°C @Thickness 1.57 mm, Temperature 20.0 °C |
8.33 µin/in-°F @Thickness 0.0620 in, Temperature 68.0 °F |
x-axis; IPC-TM 650-2.4.24 |
Industrial Laminates/Norplex NP511 Glass Fabric Description: Woven glass fabric with high temperature epoxy resin. Excellent mechanical strength and electrical properties at elevated temperatures. Continuous operating temperature is 165°C. Mat.. |
|||
CTE, linear, Transverse to Flow | 15.0 µm/m-°C @Thickness 1.57 mm, Temperature 20.0 °C |
8.33 µin/in-°F @Thickness 0.0620 in, Temperature 68.0 °F |
x-axis; IPC-TM 650-2.4.24 |
Industrial Laminates/Norplex NP630 Paper Base Laminate Description: Machining grade with good electrical properties and moisture resistance. Low cold flow with good dimensional stability. Thickness Tested: 0.062", 0.125", and 0.500" |
|||
CTE, linear, Transverse to Flow | 15.0 µm/m-°C @Thickness 1.57 mm, Temperature 20.0 °C |
8.33 µin/in-°F @Thickness 0.0620 in, Temperature 68.0 °F |
x-axis; IPC-TM 650-2.4.24 |
Industrial Laminates/Norplex NP612 Paper Base Laminate Description: Room temperature punching and shearing grade up to .125" thick. More flexible and lower mechanical properties than NP611. Intended for applications where electrical and moisture require.. |
|||
CTE, linear, Transverse to Flow | 15.0 µm/m-°C @Thickness 1.57 mm, Temperature 20.0 °C |
8.33 µin/in-°F @Thickness 0.0620 in, Temperature 68.0 °F |
x-axis; IPC-TM 650-2.4.24 |
Industrial Laminates/Norplex NP625 Paper Base Laminate Description: Paper phenolic grade with better moisture resistance than NP612. Requires less heat to punch and shear than NP611. |
|||
CTE, linear, Transverse to Flow | 15.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
8.33 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP MF002S PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MF002S is a compound based on Polypropylene resin containing Glass Fiber. Added features include: Heat Stabilized. |
|||
CTE, linear, Transverse to Flow | 15.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
8.33 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Starflam AFR470X2 PA66, 35% Glass Filled, Injection Molded AFR470X2 is a Red Phosphorous, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli.. |
|||
CTE, linear, Transverse to Flow | 15.0 µm/m-°C @Temperature 20.0 °C |
8.33 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Orgalloy® LE 6010 HV Nylon Alloy, 10% Glass Fiber Reinforced (Conditioned) LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents). 10% glass fiber reinforced. Suited to blow molding of technical pa.. |
|||
CTE, linear, Transverse to Flow | 15.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
8.33 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Dry) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
CTE, linear, Transverse to Flow | 15.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
8.33 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 11359-1/-2 |
BASF Ultramid® KR 4355 G7 BK 00564 35% Glass Filled PA6/6T (Dry) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
CTE, linear, Transverse to Flow | 15.0 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
8.33 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359-2 |
Ascend Performance Materials Vydyne® 41 Nylon 66, DAM Vydyne® 41 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
CTE, linear, Transverse to Flow | 15.0 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
8.33 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359-2 |
Ascend Performance Materials Vydyne® 41H BK03 Nylon 66, Impact Modified, DAM Vydyne® 41H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
CTE, linear, Transverse to Flow | 15.0 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
8.33 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359-2 |
Ascend Performance Materials Vydyne® 41H NT Nylon 66, Impact Modified, DAM Vydyne® 41H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyn.. |
|||
CTE, linear, Transverse to Flow | 15.0 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
8.33 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359-2 |
Ascend Performance Materials Vydyne® 41H Nylon 66, Impact Modified, DAM Vydyne® 41H is a general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne.. |
|||
CTE, linear, Transverse to Flow | 15.0 µm/m-°C @Thickness 2.00 mm, Temperature 23.0 - 55.0 °C |
8.33 µin/in-°F @Thickness 0.0787 in, Temperature 73.4 - 131 °F |
ISO 11359-2 |
Ascend Performance Materials Vydyne® 41 NT Nylon 66, Impact Modified, DAM Vydyne® 41 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |