Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 15.0 µm/m-°C
8.33 µin/in-°F
XY Direction
Premix Premi-Glas® 2206-15 CR-SX Fiberglass Reinforced Thermoset SMC
Premi-Glas® 2206-15 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f..
CTE, linear, Transverse to Flow 15.0 µm/m-°C
8.33 µin/in-°F
XY Direction
Premix Premi-Glas® 2206-22 CR-SX Fiberglass Reinforced Thermoset SMC
Premi-Glas® 2206-22 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f..
CTE, linear, Transverse to Flow 15.0 µm/m-°C
8.33 µin/in-°F
XY Direction
Premix Premi-Glas® 2206-25 CR-SX Fiberglass Reinforced Thermoset SMC
Premi-Glas® 2206-25 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f..
CTE, linear, Transverse to Flow 15.0 µm/m-°C

@Temperature 20.0 °C
8.33 µin/in-°F

@Temperature 68.0 °F
Crosswise; ASTM D696
G-11 Fiberglass Epoxy Laminate Sheet
This glass-epoxy laminate is specified for its extremely high strength and high dimensional stability over temperature. G-11 is used for terminal boards, high humidity applications, electrical and e..
CTE, linear, Transverse to Flow 15.0 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
8.33 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis; IPC-TM 650-2.4.24
Industrial Laminates/Norplex NP511 Glass Fabric
Description: Woven glass fabric with high temperature epoxy resin. Excellent mechanical strength and electrical properties at elevated temperatures. Continuous operating temperature is 165°C. Mat..
CTE, linear, Transverse to Flow 15.0 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
8.33 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis; IPC-TM 650-2.4.24
Industrial Laminates/Norplex NP630 Paper Base Laminate
Description: Machining grade with good electrical properties and moisture resistance. Low cold flow with good dimensional stability. Thickness Tested: 0.062", 0.125", and 0.500"
CTE, linear, Transverse to Flow 15.0 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
8.33 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis; IPC-TM 650-2.4.24
Industrial Laminates/Norplex NP612 Paper Base Laminate
Description: Room temperature punching and shearing grade up to .125" thick. More flexible and lower mechanical properties than NP611. Intended for applications where electrical and moisture require..
CTE, linear, Transverse to Flow 15.0 µm/m-°C

@Thickness 1.57 mm,
Temperature 20.0 °C
8.33 µin/in-°F

@Thickness 0.0620 in,
Temperature 68.0 °F
x-axis; IPC-TM 650-2.4.24
Industrial Laminates/Norplex NP625 Paper Base Laminate
Description: Paper phenolic grade with better moisture resistance than NP612. Requires less heat to punch and shear than NP611.
CTE, linear, Transverse to Flow 15.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
8.33 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP MF002S PP (Europe-Africa-Middle East)
LNP* THERMOCOMP* MF002S is a compound based on Polypropylene resin containing Glass Fiber. Added features include: Heat Stabilized.
CTE, linear, Transverse to Flow 15.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
8.33 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Starflam AFR470X2 PA66, 35% Glass Filled, Injection Molded
AFR470X2 is a Red Phosphorous, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
CTE, linear, Transverse to Flow 15.0 µm/m-°C

@Temperature 20.0 °C
8.33 µin/in-°F

@Temperature 68.0 °F
Arkema Group Orgalloy® LE 6010 HV Nylon Alloy, 10% Glass Fiber Reinforced (Conditioned)
LE series, flexible polyamide alloys: processability on PE screw, low moisture absorption, chemical resistance (no known solvents). 10% glass fiber reinforced. Suited to blow molding of technical pa..
CTE, linear, Transverse to Flow 15.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
8.33 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 11359-1/-2
BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Dry)
Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r..
CTE, linear, Transverse to Flow 15.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
8.33 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 11359-1/-2
BASF Ultramid® KR 4355 G7 BK 00564 35% Glass Filled PA6/6T (Dry)
Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r..
CTE, linear, Transverse to Flow 15.0 µm/m-°C

@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
8.33 µin/in-°F

@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® 41 Nylon 66, DAM
Vydyne® 41 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp..
CTE, linear, Transverse to Flow 15.0 µm/m-°C

@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
8.33 µin/in-°F

@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® 41H BK03 Nylon 66, Impact Modified, DAM
Vydyne® 41H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd..
CTE, linear, Transverse to Flow 15.0 µm/m-°C

@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
8.33 µin/in-°F

@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® 41H NT Nylon 66, Impact Modified, DAM
Vydyne® 41H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyn..
CTE, linear, Transverse to Flow 15.0 µm/m-°C

@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
8.33 µin/in-°F

@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® 41H Nylon 66, Impact Modified, DAM
Vydyne® 41H is a general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne..
CTE, linear, Transverse to Flow 15.0 µm/m-°C

@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
8.33 µin/in-°F

@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
ISO 11359-2
Ascend Performance Materials Vydyne® 41 NT Nylon 66, Impact Modified, DAM
Vydyne® 41 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im..