Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 27.0 - 100 µm/m-°C
15.0 - 55.6 µin/in-°F
Average value: 51.2 µm/m-°C Grade Count:10
Overview of materials for Acetal Copolymer, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va..
CTE, linear, Transverse to Flow 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
XY-direction; ASTM D696
Premix Premi-Glas® 1265 VE 1265-VE (Compression Molded) Glass Reinforced Vinyl Ester TMC  (discontinued **)<
Description: Premi-Glas® 1265 VE is a glass reinforced vinyl ester molding compound designed for automotive under the hood applications. Key features and benefits: Designed for Injection or Injecti..
CTE, linear, Transverse to Flow 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
XY-direction; ASTM D696
Premix Premi-Glas® 1265 VE 1265-VE (Injection Compression Molded) Glass Reinforced Vinyl Ester TMC  (discontin
Description: Premi-Glas® 1265 VE is a glass reinforced vinyl ester molding compound designed for automotive under the hood applications. Key features and benefits: Designed for Injection or Injecti..
CTE, linear, Transverse to Flow 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
XY-direction; ASTM D696
Premix Premi-Glas® 2200-22 Fiberglass Reinforced SMC  (discontinued **)
Description: Premi-Glas® 2200-22 is a fiberglass reinforced thermoset Sheet Molding Compound similar to the Premi-Glas® 2200-22 CR-SX product. Unlike the -CR-SX version, this product carries no UL..
CTE, linear, Transverse to Flow 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
XY-direction; ASTM D696
Premix Premi-Glas® 8102-13 Glass Reinforced Polyester BMC  (discontinued **)
Description: Premi-Glas® 8102-13 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits:..
CTE, linear, Transverse to Flow 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
XY-direction; ASTM D696
Premix Premi-Glas® 8102-20 Glass Reinforced Polyester BMC  (discontinued **)
Description: Premi-Glas® 8102-20 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits:..
CTE, linear, Transverse to Flow 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
XY-direction; ASTM D696
Premix Premi-Glas® 8105 Glass Reinforced Polyester BMC  (discontinued **)
Description: Premi-Glas® 8105 is a glass reinforced thermoset polyester Bulk Molding Compound designed for injection molding of automotive forward lighting reflectors. Key features and benefits: Ex..
CTE, linear, Transverse to Flow 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
XY-direction; ASTM D696
Premix Premi-Glas® 8201-24 Glass Reinforced Polyester SMC  (discontinued **)
Description: Premi-Glas® 8201-24 is a low profile glass reinforced polyester Sheet Molding Compound designed for body panel applications.Key features and benefits: Compatible with in-mold coatings,..
CTE, linear, Transverse to Flow 27.0 µm/m-°C

@Temperature -20.0 - 150 °C
15.0 µin/in-°F

@Temperature -4.00 - 302 °F
ASTM E 831
SABIC Innovative Plastics ULTEM 2312 PEI
30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.
CTE, linear, Transverse to Flow 27.0 µm/m-°C

@Temperature -20.0 - 150 °C
15.0 µin/in-°F

@Temperature -4.00 - 302 °F
ASTM E 831
SABIC Innovative Plastics ULTEM 2312 PEI (Asia Pacific)
30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.
CTE, linear, Transverse to Flow 27.0 µm/m-°C

@Temperature 23.0 - 150 °C
15.0 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
SABIC Innovative Plastics ULTEM 2312 PEI (Europe-Africa-Middle East)
30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing.
CTE, linear, Transverse to Flow 27.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
15.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP EX93452 PEI
LNP THERMOCOMP* EX93452 is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Electrically Conductive.
CTE, linear, Transverse to Flow 27.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
15.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP UFW49S PPA
LNP* THERMOCOMP* UFW49S is a compound based on Polyphthalamide resin containing 45% Glass Fiber, 20% Wollastonite. Added features of this material include: Heat Stabilized, Low Warpage.
CTE, linear, Transverse to Flow 27.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
15.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP JCL36E PES
LNP* LUBRICOMP* JCL36E is a compound based on Polyethersulfone (PES) resin containing 30% Carbon Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant.
CTE, linear, Transverse to Flow 27.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
15.0 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP UX04509 PPA
LNP* Thermocomp* UX04509 is a compound based on Polyphthalamide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
CTE, linear, Transverse to Flow 27.0 µm/m-°C
15.0 µin/in-°F
TMA
Vyncolit Vyntec® CF8131 Carbon Fiber Reinforced Phenolic
VYNTEC CF8050 is a carbon fiber reinforced phenolic moldable composite with good tribological and superior mechanical properties combined with low density. Very good chemical resistance in several o..
CTE, linear, Transverse to Flow 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
XY-direction; ASTM D696
Premix Premi-Glas® 1282-32 VE Glass Reinforced Vinyl Ester SMC  (discontinued **)
Description: Premi-Glas® 1282-32 VE SMC is an enhanced high strength glass reinforced vinyl ester molding compound formulated for under-the-hood automotive applications. Key features and benefi..
CTE, linear, Transverse to Flow 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
XY-direction; ASTM D696
Premix Premi-Glas® 1281-32 VE Glass Reinforced Vinyl Ester SMC  (discontinued **)
Description: Premi-Glas® 1281-32 VE SMC is a high strength glass reinforced vinyl ester sheet molding compound formulated for under-the-hood automotive applications. Key features and benefits: Desi..
CTE, linear, Transverse to Flow 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
XY-direction
Premix Premi-Glas® 7203-28 28% Glass Reinforced Polyester SMC  (discontinued **)