Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 36.5 µm/m-°C @Temperature -30.0 - 30.0 °C |
20.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics LNP Thermocomp LFZ42XXC PEEK LNP THERMOCOMP* LFZ42XXC is a compound based on Polyetheretherketone resin containing Glass Fiber, Milled Glass. Added features of this material include: Low Warpage.This data was supplied by SABIC.. |