CTE, linear, Transverse to Flow 36.5 µm/m-°C

@Temperature -30.0 - 30.0 °C
20.3 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D 696
SABIC Innovative Plastics LNP Thermocomp LFZ42XXC PEEK
LNP THERMOCOMP* LFZ42XXC is a compound based on Polyetheretherketone resin containing Glass Fiber, Milled Glass. Added features of this material include: Low Warpage.This data was supplied by SABIC..