Polymer Property : CTE, linear, Transverse to Flow = 30.6 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 6.00 - 55.0 µm/m-°C
3.33 - 30.6 µin/in-°F
Average value: 47.4 µm/m-°C Grade Count:38
Overview of materials for Polyimide
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
CTE, linear, Transverse to Flow 55.0 - 55.0 µm/m-°C

@Temperature 200 - 200 °C
30.6 - 30.6 µin/in-°F

@Temperature 392 - 392 °F
Average value: 55.0 µm/m-°C Grade Count:1
Overview of materials for Thermoplastic Polyimide, Unfilled
CTE, linear, Transverse to Flow 26.8 - 55.0 µm/m-°C
14.9 - 30.6 µin/in-°F
Average value: 39.8 µm/m-°C Grade Count:22
Overview of materials for Phenolic, Novolac, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Glass Filled". Each property range of values reported is minimum and maximum values o..
CTE, linear, Transverse to Flow 40.0 - 55.0 µm/m-°C
22.2 - 30.6 µin/in-°F
Average value: 44.3 µm/m-°C Grade Count:7
Overview of materials for Nylon 66, 60% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. ..